P235GH is the base non-alloy grade of EN 10216-2, the part of the pressure tube standard written for elevated temperature service. It is the European counterpart of ASTM A106 Grade B and the grade that most boiler and pressure equipment in Europe is still designed around: 235 MPa yield, 360–500 MPa tensile, normalized delivery, 27 J impact at 20 °C, and a table of 0.2% proof stress values up to 400 °C. It is not a high-temperature alloy. Above roughly 350 °C the allowable stress falls sharply, and above 400 °C there is no tabulated data at all — that is where 16Mo3 and 13CrMo4-5 take over. The distinction between P235GH and P235TR2 is design basis, not appearance.
What the standard actually guarantees
Table 1 — Scope of EN 10216-2 for P235GH
| Item | Requirement | Practical meaning |
|---|---|---|
| Service | Elevated temperature pressure purposes | Design must use the standard’s proof stress table, not the room-temperature yield |
| Delivery condition | Normalized (N) | Air cooled from 900–950 °C; uniform ferrite-pearlite |
| Tabulated temperature range | 20 – 400 °C | Above 400 °C there is no design data in the standard |
| Impact | 27 J at 20 °C | Not a low-temperature grade; use EN 10216-4 below 0 °C |
| Certificate | EN 10204 3.1 | Heat number, chemistry, tensile, impact, heat treatment record |
Chemical composition
Table 2 — Chemical requirements, heat analysis (%)
| Element | Requirement | Note |
|---|---|---|
| Carbon | 0.16 max | Lower carbon improves weldability and toughness |
| Silicon | 0.35 max | Deoxidation |
| Manganese | 0.40 – 1.20 | Strength and deoxidation |
| Phosphorus | 0.025 max | Restricted for toughness |
| Sulphur | 0.020 max | Restricted for weldability |
| Aluminium, total | 0.020 min | Fine grain practice; the difference between GH and TR |
| Chromium | 0.30 max | Residual |
| Copper | 0.30 max | Residual |
| Nickel | 0.30 max | Residual |
| Molybdenum | 0.08 max | Residual; above this it becomes a Mo grade |
| Niobium | 0.010 max | Residual |
| Titanium | 0.040 max | Residual |
| Vanadium | 0.02 max | Residual |
Mechanical properties
Table 3 — Room-temperature requirements
| Property | Requirement | Note |
|---|---|---|
| Yield, 0.2% | 235 MPa min | Reduces above 16 mm wall |
| Tensile | 360 – 500 MPa | The upper limit is enforced |
| Elongation in 50 mm | 25% min | — |
| Impact, Charpy V | 27 J at 20 °C | Transverse where wall allows |
| Hardness | Not specified | Typically 140–165 HBW |
| Grain size | Fine grain, Al-killed | Required for the elevated-temperature data to apply |
Elevated-temperature design
EN 10216-2 tabulates the 0.2% proof stress for P235GH from 20 to 400 °C. The values fall steadily: by 300 °C the proof stress is roughly three quarters of the room-temperature yield, and by 400 °C roughly two thirds. Above 400 °C the standard is silent, which is the point at which the design has to move to 16Mo3 or 13CrMo4-5 if the temperature cannot be reduced.
Table 4 — Design range and where the next grade starts
| Parameter | Value |
|---|---|
| Tabulated proof stress range | 20 – 400 °C (EN 10216-2 Table 5) |
| Typical boiler service | Up to 350 °C steam; economiser and lower waterwall |
| Practical ceiling | 400 °C, where the tabulated data ends |
| Next grade up | 16Mo3 to 500 °C, then 13CrMo4-5 to 530 °C |
| Low-temperature limit | 0 °C for the standard impact test; below that EN 10216-4 |
P235GH against P265GH and A106 B
Table 5 — Grade selection for a pressure tube
| P235GH | P265GH | A106 Gr.B | |
|---|---|---|---|
| Standard | EN 10216-2 | EN 10216-2 | ASTM A106 |
| Yield | 235 MPa | 265 MPa | 240 MPa |
| Tensile | 360 – 500 MPa | 410 – 530 MPa | 415 MPa min |
| Impact | 27 J at 20 °C | 27 J at 20 °C | Not standard |
| Elevated data | To 400 °C | To 400 °C | ASME table to 538 °C |
| Typical use | Boiler and vessel, European code | Higher pressure at the same wall | US code piping and boiler |
Sizes and tolerances
Table 6 — Dimensional range
| Parameter | Range / tolerance |
|---|---|
| Outside diameter | 10.2 – 762 mm |
| Wall thickness | 1.6 – 100 mm |
| OD tolerance | ±0.75% or ±0.5 mm (D2) |
| Wall tolerance | −12.5% / +15% (S2), or ±10% (S1) |
| Length | 5 – 7 m random, or fixed 3 – 12 m |
| Straightness | 0.2% of length |
| Ends | Plain, bevelled, or threaded |
Where P235GH is used
Boiler waterwalls
Membrane wall and lower furnace tubes where the metal temperature stays below 400 °C and the pressure is moderate.
Economisers
Feedwater heating banks, where the tube is finned or bare and the duty is below the creep range.
Steam headers
Low-pressure and saturated steam headers, flanged and welded, with normalized tube and a 3.1 certificate.
Pressure vessels
Shell and nozzle tube in small vessels built to EN 13445, where P235GH is the default plate and tube grade.
Heat exchangers
Shell-side and low-temperature tube bundles in process duty without chlorides.
Piping spools
Steam and condensate lines in plant distribution, where A106 B is unavailable and the European grade is specified.
Frequently asked questions
What is the maximum temperature for P235GH?
400 °C, which is where EN 10216-2 stops tabulating proof stress. In practice most boiler designs switch to 16Mo3 above about 400 °C and to 13CrMo4-5 above 480 °C, because the carbon steel wall becomes uneconomical before it becomes unsafe.
Is P235GH the same as P235TR2?
No. P235TR2 is EN 10216-1 for room-temperature service with 27 J at 0 °C; P235GH is EN 10216-2 for elevated temperature, normalized, with 27 J at 20 °C and proof stress data to 400 °C. Same yield, different design basis and different standard.
Can P235GH replace A106 Grade B?
In many European designs, yes, and the reverse is often accepted too. They are close but not identical: P235GH has a guaranteed 235 MPa yield with mandatory impact testing and fine grain practice, while A106 B has 240 MPa and no standard impact requirement. The substitution needs design approval.
Why is aluminium specified as a minimum?
Aluminium addition produces fine grain steel, which is what gives P235GH its toughness and its elevated-temperature proof stress. A heat with aluminium below 0.020% does not meet the standard, and the tube cannot be certified to EN 10216-2 whatever its tensile results.
What is the difference between P235GH and P265GH?
Yield: 235 against 265 MPa, with tensile 360–500 against 410–530 MPa. P265GH is chosen when the design pressure will not close in P235GH at an economic wall. Both are normalized and both are tabulated to 400 °C.
Can P235GH be supplied in the cold drawn condition?
Yes, cold drawn tube is normalized after drawing to meet the delivery condition. Cold drawn plus normalized gives tighter dimensional tolerance than hot finished, at a higher price. State the tolerance class as well as the grade.
Is impact testing at lower temperature available?
Yes, by agreement, but the grade is not designed for it. If the design temperature is below 0 °C, EN 10216-4 grades such as P215NL or P265NL are the correct choice rather than a special P235GH.
What is the minimum order and lead time?
1 tonne per size for standard dimensions. Lead time is 15–25 days; larger diameters and non-standard walls run longer. Third-party inspection adds about a week.
Request a quote
Related products
P265GH (1.0425) TubeHigher strength EN 10216-2 grade
16Mo3 Tube0.3% Mo for service to 500 °C
13CrMo4-5 Tube1.25Cr-0.5Mo for service to 530 °C
DIN 17175 PipeThe legacy German standard
ASTM A106 PipeThe US carbon steel pressure pipe
All boiler and pressure tube · Guide: the five parts of EN 10216 and how to read a pressure tube drawing
Also in this range: P235TR2 (1.0255) pressure tube · DIN 17175 boiler pipe · EN 10297-1 E355 mechanical tube · EN 10297-1 E275 mechanical tube.
Request a quotation
Give us OD, wall, length, quantity, design temperature and whether impact testing above the standard 20 °C is required. Tell us the design code if the tube is for a coded vessel.