Project Description

P265GH 1.0425 seamless pressure tube to EN 10216-2, normalized, bundled with heat number stencil
10 – 610 mmoutside diameter
to 60 mmwall thickness
265 MPayield at 16 mm
410 – 570 MPatensile
450 °Celevated data
EN 10204 3.1mill certificate
MOQ 1 tonne per size
Lead time 15–25 days
Test category TC1 / TC2
Quote within 24 hours
Impact 40 J at +20 °C
Need P265GH with impact data? Send OD, wall, quantity and test category — quotation back within 24 hours.
Get a quote

P265GH — EN number 1.0425 — is the non-alloy elevated-temperature pressure tube grade of EN 10216-2, sitting one step above P235GH with a guaranteed minimum yield of 265 MPa across the same temperature envelope. That extra 30 MPa is the whole reason it exists: it lets a designer hold a wall thickness that would otherwise have to grow, on boiler tubes, header stubs, feedwater and steam lines, and pressure vessel nozzles. Two things separate it from ordinary carbon pipe. It is aluminium-killed fine grain steel, so it keeps toughness after normalizing, and it carries mandatory impact testing with elevated-temperature proof strength published to 450 °C. We supply it normalized in test category TC1 or TC2, OD 10 to 610 mm, with the chemical, tensile, impact and high-temperature values on an EN 10204 3.1 certificate.

Why P265GH rather than ordinary carbon steel

EN 10216-2 does not simply rename a carbon steel. The grade requires fully killed steel with a minimum aluminium content of 0.020%, which pins the grain size and keeps the impact transition temperature low after normalizing. It also caps the residual elements collectively — Cr + Cu + Mo + Ni not exceeding 0.70% — because those residuals are what make a heat brittle or unpredictable in elevated-temperature service.

The practical consequence: a P265GH tube can be normalized, impact tested and welded without the fabricator having to qualify a special procedure, and it will still hold its guaranteed proof strength at 300 °C. A commercial carbon tube cannot promise either.

Chemical composition

Table 1 — P265GH / 1.0425 chemistry, cast analysis (%)

Element Requirement Element Requirement
C 0.20 max Al, total 0.020 min
Si 0.40 max Cu 0.30 max
Mn 1.40 max Nb 0.010 max
P 0.025 max Ti 0.040 max
S 0.020 max V 0.02 max
Cr 0.30 max Cr + Cu + Mo + Ni 0.70 max
Mo 0.080 max Ni 0.30 max

Aluminium is the line that matters. A heat at 0.015% Al may pass every mechanical test and still fail the specification — and it will behave differently in the heat-affected zone. Ask for the Al value on the certificate, not just the tensile result.

Mechanical properties

Table 2 — Room temperature tensile and yield by wall thickness

Wall thickness Yield ReH min Tensile Rm Elongation A min (longitudinal / transverse)
Up to 16 mm 265 MPa 410 – 570 MPa 23% / 21%
Over 16 – 40 mm 255 MPa 410 – 570 MPa 23% / 21%
Over 40 – 60 mm 245 MPa 410 – 570 MPa 23% / 21%

Table 3 — Impact properties, minimum average absorbed energy

Test temperature Longitudinal Transverse Note
+20 °C 40 J 28 J The default test for TC1 and TC2
0 °C 27 J — Quoted when the design temperature is low
−10 °C On request — Needs to be specified; not part of the base grade

Impact values are minimum averages for a set of three specimens, with a single value allowed to fall below the average but not below 70% of it. If your specification calls for a lower test temperature than 0 °C, say so at enquiry — it changes the heat treatment route and the price.

Proof strength at elevated temperature

This is the table the boiler designer actually uses. Note that the guaranteed strength falls roughly 40% between 100 °C and 450 °C, which is why a line sized on room-temperature yield will be under-designed at temperature.

Table 4 — Minimum proof strength Rp0.2 at temperature, wall up to 60 mm

Temperature Rp0.2 min Temperature Rp0.2 min
100 °C 226 MPa 350 °C 141 MPa
150 °C 213 MPa 400 °C 134 MPa
200 °C 192 MPa 450 °C 128 MPa
250 °C 171 MPa 500 °C Not specified
300 °C 154 MPa 550 °C Not specified

The table stops at 450 °C because that is where the standard stops. Above 450 °C the design needs a creep-resisting grade — 16Mo3 or 13CrMo4-5 — not a thicker carbon wall.

Heat treatment

Table 5 — Normalizing conditions

Condition Austenitizing temperature Cooling Tempering
+N (normalized) 880 – 940 °C Air None
+N with normalizing forming 880 – 940 °C Air None — permitted by the standard

Normalizing forming means the final forming operation is done at normalizing temperature and the part is then allowed to cool in air, so no separate reheat is needed. It is common for header stubs and bends and has to be declared on the order.

Standards and equivalents

Table 6 — P265GH against the specifications it is compared with

System Designation Product form Difference
EN EN 10216-2 — P265GH / 1.0425 Seamless pressure tube Reference specification for this page
EN EN 10217-2 — P265GH Welded pressure tube Electric welded version; same grade name, different product
ASTM A106 Grade B Seamless pipe Closest US equivalent. 240 MPa yield against 265 MPa — not interchangeable without review
ASTM A516 Grade 70 Plate Same strength class for vessel shells and tube sheets
JIS JIS G3456 STPT410 High temperature pipe Japanese equivalent grade
GB GB 5310 20G / GB/T 3087 20# Boiler tube / low pressure pipe 20G is the closer match; 20# has no elevated temperature data
DIN DIN 17175 St45.8 Seamless tube Withdrawn, superseded by EN 10216-2

The most common substitution request we see is A106 B in place of P265GH. It usually passes on tensile and fails on yield — 240 against 265 MPa — and it has no aluminium requirement. For a European pressure vessel that is normally enough to stop the substitution.

Inspection and test category

Table 7 — What is tested, and what TC2 adds

Test TC1 TC2 Notes
Cast analysis Required Required On the certificate either way
Tensile at room temperature Required Required Yield, tensile, elongation
Impact test Required Required +20 °C as standard
Flattening / ring test Required Required Per size and wall
Leak tightness (hydrostatic) Required Required Or NDT by agreement
Dimensional and visual Required Required —
Product analysis Optional Required Confirms the finished tube, not just the cast
NDT of the tube body Not required Required Eddy current or ultrasonic
Elevated temperature tensile Optional Optional Ordered when the design needs verified data

Where P265GH is the right answer

Boiler waterwall and economiser

Furnace wall tubes and economiser sections where the metal temperature stays under 400 °C and carbon steel creep is not yet the governing case.

Header stubs and nozzles

Short thick-wall connections into drums and headers. The 265 MPa yield holds the wall down where a P235GH design would grow.

Feedwater and steam lines

Low and medium pressure steam and feedwater piping in combined heat and power and industrial boiler plants.

Pressure vessel shells

Shell courses and end closures where EN 10028-2 P265GH plate is used and the tube specification has to match the plate.

Heat exchanger shells

Shell-side service in the 200–400 °C band, particularly where a notified body requires documented elevated temperature data.

Air receiver and accumulator

Compressed air and nitrogen vessels built to the pressure equipment directive, where TC2 and a 3.1 certificate are the default expectation.

Frequently asked questions

What is the difference between P265GH and P235GH?

Thirty megapascals of guaranteed yield — 265 against 235 — and the same temperature envelope up to 450 °C. The choice is purely a wall thickness question: if the P235GH design needs a wall the fabricator considers excessive, P265GH closes it without changing anything else on the line.

Can A106 Grade B replace P265GH?

Rarely without a review. A106 B guarantees 240 MPa yield against 265 MPa, has no aluminium-killed fine grain requirement and no mandatory impact test. On a European pressure vessel that combination usually fails the design check at the first review.

What does test category TC1 and TC2 mean in practice?

TC2 adds NDT of the tube body and a product analysis on the finished tube. For boiler and pressure equipment in Europe, TC2 is the normal order; TC1 appears on less critical or non-notified work. If the enquiry does not state a category, we will ask before quoting.

At what temperature does P265GH stop being suitable?

The standard publishes proof strength to 450 °C, and that is the practical ceiling. Above it the design has to consider creep, which means 16Mo3 or 13CrMo4-5 rather than more carbon steel.

Is P265GH the same as P265GH to EN 10217-2?

The grade is the same, the product is not. EN 10216-2 is seamless, EN 10217-2 is electric welded. They are separate specifications with separate test schedules and cannot be certified as each other.

Is it always normalized?

Normalizing is the standard delivery condition, and normalizing forming is permitted. As-rolled supply exists in the market but should be treated with suspicion unless the mill can show the mechanical properties and impact results for the actual condition supplied.

What certificate and marking do you supply?

EN 10204 3.1 with heat number, cast and product analysis, tensile, yield, elongation, impact energy and the test temperature. Marking is stencilled or stamped on each length with grade, size, heat number and the manufacturer’s mark, and repeated on the bundle tag.

What is the minimum order and lead time?

One tonne per size. Lead time 15–25 days; TC2 with third-party inspection adds about a week, and diameters above 400 mm run longer because fewer mills roll them.

Send the pressure class and the design temperature. That is enough for us to confirm the grade, the test category and the impact requirement before quoting — and to say so if a creep-resisting grade is the better answer.
Request a quote
WhatsApp

Related products

All boiler and pressure tube — carbon, alloy and stainless · Guide: which standard governs your order

Request a quotation

Tell us OD, wall, quantity, design temperature and the test category you need. We reply within 24 hours with price, lead time and certificate scope — and we will query an impact temperature that the grade cannot meet before you order.

    Your Name *

    Your Email *

    Company Name

    Phone / WhatsApp *

    Grade & Standard (e.g. ASTM A106 Gr.B, EN 10216-2 P265GH)

    Size, OD × WT (e.g. 88.9 × 5.49 mm)

    Quantity & Unit (e.g. 500 m / 20 t)

    Destination Port

    Drawing or Datasheet (pdf, dwg, step, xlsx; max 5 MB)

    Further Information