Project Description

10CrMo9-10 1.7380 2.25Cr-1Mo alloy seamless pressure tube, normalized, for main steam piping
10 – 600 mmoutside diameter
1 – 80 mmwall thickness
2.0 – 2.5%chromium
0.9 – 1.1%molybdenum
580 °Cservice ceiling
EN 10204 3.1mill certificate
MOQ 1 tonne per size
Lead time 30–40 days
Test category TC1 / TC2
Quote within 24 hours
Third party SGS / BV / TUV
Main steam above 540 °C? Send OD, wall, temperature and quantity — quotation back within 24 hours.
Get a quote

10CrMo9-10 — EN number 1.7380, the 2.25% chromium, 1% molybdenum grade — is the next step up from 13CrMo4-5 in the creep-resisting family. Where the 1.25Cr steel runs out at about 550 °C, 2.25Cr-1Mo carries main steam piping, headers and hydrogen-bearing process lines into the 550–580 °C band, and it does so with better resistance to hydrogen attack, which is why refining and ammonia service reach for it. It is supplied normalized and welded with preheat and post-weld heat treatment; the PWHT temperature matters more here than on 13CrMo4-5 because the alloy is more sensitive to over-tempering. We supply OD 10 to 600 mm, wall 1 to 80 mm, in TC1 or TC2, with elevated-temperature proof strength on the certificate.

Where it sits in the creep ladder

Table 1 — Selecting by design metal temperature

Design temperature Grade Why
Up to 400 °C P265GH No alloy premium justified
400 – 480 °C 16Mo3 0.3% Mo lifts creep strength cheaply
480 – 550 °C 13CrMo4-5 1.25Cr-0.5Mo, the standard superheater grade
550 – 580 °C 10CrMo9-10 2.25Cr-1Mo; higher creep rupture strength at the same wall
Above 580 °C T91 / P91 9Cr martensitic; the ferritic grades no longer hold

The other reason to choose 2.25Cr-1Mo is hydrogen. Above about 450 °C and at hydrogen partial pressure, carbon steel and even 1.25Cr suffer hydrogen attack; the Nelson curves place 2.25Cr-1Mo in a much safer band, which is why hydrotreaters and ammonia plants are built from it.

Chemical composition

Table 2 — 10CrMo9-10 / 1.7380 chemistry, cast analysis (%)

Element Requirement Element Requirement
C 0.08 – 0.14 P 0.020 max
Si 0.50 max S 0.010 max
Mn 0.40 – 0.80 Cr 2.00 – 2.50
Mo 0.90 – 1.10 — —

Carbon is capped at 0.14% — lower than 13CrMo4-5 — because at 2.25% chromium a higher carbon content promotes carbide coarsening and embrittlement in thick sections. Sulphur at 0.010% is mandatory for weldability.

Mechanical properties

Table 3 — Tensile and yield by wall thickness, normalized

Wall thickness Tensile Rm Yield ReH min
Up to 16 mm 480 – 630 MPa 310 MPa
Over 16 – 40 mm 480 – 630 MPa 300 MPa
Over 40 – 60 mm 480 – 630 MPa 290 MPa
Over 60 – 100 mm 470 – 620 MPa 280 MPa
Over 100 – 150 mm 460 – 610 MPa 260 MPa
Over 150 – 250 mm 450 – 600 MPa 250 MPa

Welding and heat treatment

Table 4 — Thermal practice

Item Value Note
Normalizing (+N) 900 – 960 °C, air cool Standard delivery condition
Preheat before welding 200 – 300 °C Higher than for 1.25Cr; the hardenability is greater again
Interpass temperature 300 °C maximum Excess heat input coarsens the HAZ
Post-weld heat treatment 690 – 750 °C Hold 1 h per 25 mm; do not exceed 750 °C
Filler metal 2.25Cr-1Mo matching (e.g. ER90S-B3 / E9018-B3) Carbon or 1.25Cr filler is not correct
Hardness after PWHT 250 HV10 maximum in the HAZ Confirm on the procedure qualification

The one failure mode to watch: PWHT above 750 °C. It looks like being thorough, but it over-tempers the steel and the creep rupture life drops without any visible change. The fabricator’s procedure should state the ceiling, not just the target.

Standards and equivalents

Table 5 — Cross-reference

System Designation Product form
EN EN 10216-2 — 10CrMo9-10 / 1.7380 Seamless tube
ASTM A335 P22 Seamless pipe
ASTM A213 T22 Boiler and heat exchanger tube
ASTM A387 Gr.22 Plate
JIS STPA24 / STBA24 Pipe / tube
GB GB 5310 10CrMo910 Boiler tube
DIN DIN 17175 10CrMo910 Withdrawn predecessor

Where 10CrMo9-10 is used

Main steam piping

Subcritical and supercritical main steam and hot reheat lines in the 550–580 °C band, where 1.25Cr has run out of creep strength.

Boiler headers

Header bodies and stubs at the top of the superheater, where the metal temperature is highest and the wall is thickest.

Hydrotreaters and hydrocrackers

Hydrogen-bearing process lines and reactor internals, where the Nelson curves exclude lower-chrome steels.

Ammonia synthesis

High pressure synthesis loops, where 2.25Cr-1Mo is the established material for hydrogen and nitrogen service.

High pressure heat exchangers

Tube and shell in hydrogen service, where the tubes and tube sheet must both resist hydrogen attack.

Coal gasification

Hot high pressure syngas lines, one of the few duties where even 2.25Cr is pushed to its limit.

Frequently asked questions

Is 10CrMo9-10 the same as A335 P22?

Same alloy family and normally accepted as alternatives after review. The chemistry windows, tolerances and test schedules differ, and the certificate has to be re-issued against whichever standard the drawing cites.

What is the maximum service temperature?

About 580 °C, with the exact limit set by the allowable stress in the design code. Above that a 9Cr steel is required — the ferritic grades lose creep strength faster than the wall can compensate.

Why is PWHT so critical on this grade?

Because 2.25Cr-1Mo is more sensitive to tempering than 1.25Cr. Too low and the HAZ stays hard and crack-prone; too high and the creep rupture life is reduced with no visible change. The window is 690–750 °C and it should be controlled, not approximated.

Can it be used in hydrogen service?

Yes, and that is one of its main advantages. The Nelson curves allow 2.25Cr-1Mo at hydrogen partial pressures and temperatures where carbon steel and 1.25Cr would suffer hydrogen attack. Confirm against the current curve for your conditions.

Is it supplied normalized or quenched and tempered?

Normalized as standard for tube. Quenched and tempered plate is available for heavier sections; for tube the normalized condition is the norm and what the mechanical table assumes.

Does it need impact testing?

Per test category — TC1 or TC2 both require impact. State the test temperature if it is below ambient; the base grade is normally tested at room temperature.

How does it compare with T91?

T91 carries roughly twice the allowable stress at 580 °C, so the wall is much thinner. The trade is weldability — T91 needs far tighter procedure control and is much less forgiving on site. Below 580 °C, 2.25Cr usually wins on total cost.

What is the minimum order and lead time?

One tonne per size. Lead time is 30–40 days; heavy wall and TC2 with third-party witness run towards the longer end.

Send the design temperature and the hydrogen partial pressure. Those two numbers decide whether 2.25Cr is enough or whether the duty needs a 9Cr steel. We will confirm before quoting.
Request a quote
WhatsApp

Related products

All boiler and pressure tube — carbon, alloy and stainless · Guide: which standard governs your order

Request a quotation

Give us OD, wall, design temperature, quantity and test category. We reply within 24 hours with price, lead time and certificate scope.

    Your Name *

    Your Email *

    Company Name

    Phone / WhatsApp *

    Grade & Standard (e.g. ASTM A106 Gr.B, EN 10216-2 P265GH)

    Size, OD × WT (e.g. 88.9 × 5.49 mm)

    Quantity & Unit (e.g. 500 m / 20 t)

    Destination Port

    Drawing or Datasheet (pdf, dwg, step, xlsx; max 5 MB)

    Further Information