Project Description

Monel 400 N04400 2.4360 nickel copper alloy pipe and tube for seawater and HF service
N04400 / 2.4360UNS and EN
63% minnickel
28 – 34%copper
195 / 550 MPayield / tensile
480 °Cservice ceiling
OD 6 – 219 mmtube range
MOQ 200 kg per size
Lead time 25–40 days
Third party SGS / BV / TUV
Quote within 24 hours
Certificate EN 10204 3.1 + PMI
Handling hydrofluoric acid or seawater? Send the concentration, temperature and aeration — Monel 400 is the best answer for HF and a poor one for aerated stagnant seawater.
Get a quote

Monel 400 — UNS N04400, W.-Nr. 2.4360 — is a nickel-copper alloy with about 63% nickel and 30% copper, and it occupies a corrosion niche that no stainless steel fills: hydrofluoric acid, deaerated sulphuric acid, caustic soda, and seawater where the flow is high enough to prevent stagnation. It is soft by alloy standards, 195 MPa yield, and it work-hardens rather than responds to heat treatment. That softness is an advantage in HF service because it resists erosion and does not catalyse the reactions that attack stainless. It is also the alloy behind a lot of marine hardware — pump shafts, valve trim, fasteners — where 316 fails by pitting and copper-nickel is not strong enough.

Chemistry

Table 1 — Chemical composition, ASTM B165 / EN 2.4360 (%, limits)

Element Requirement Function
Nickel 63.0 min Base; resistance to HF and caustic
Copper 28.0 – 34.0 Seawater resistance and strength
Iron 2.5 max Residual
Manganese 2.0 max Deoxidation
Carbon 0.30 max Residual; kept low for ductility
Silicon 0.50 max Residual
Sulphur 0.024 max Restricted for weldability

Mechanical properties

Table 2 — Room-temperature requirements, annealed

Property Requirement Note
Yield, 0.2% 195 MPa min Soft; cold work raises it
Tensile 550 MPa min —
Elongation in 50 mm 35% min Very ductile
Hardness ≤ 75 HRB typical —
Annealing 870 – 980 °C, water or air quench Required after cold work for corrosion service
Service ceiling 480 °C in air Above that, oxidation and creep limit it

Corrosion: the HF alloy

Table 3 — Where Monel 400 works and where it does not

Medium Performance Comment
Hydrofluoric acid, all concentrations Excellent The reference material for HF alkylation and HF handling
Seawater, flowing Good Resists pitting if velocity stays above about 1 m/s
Seawater, stagnant or polluted Poor Pitting and crevice attack; use 90-10 CuNi or 625 instead
Caustic soda Excellent Better than stainless at high concentration and temperature
Dilute sulphuric acid, deaerated Good Attacked if aerated; 904L better in aerated acid
Nitric acid and oxidizing salts Poor Rapid attack; use 304L or 310
Ammonia Good, with stress relief Stress corrosion cracking risk in anhydrous ammonia
High-temperature sulphur Poor Above 300 °C sulphidation is rapid

Monel 400 against 625 and 90-10 CuNi

Table 4 — Alloy selection for seawater and HF

Monel 400 Inconel 625 90-10 CuNi
Nickel 63 min 58 min 10
Yield 195 MPa 415 MPa 130 MPa
HF acid Best Good Poor
Flowing seawater Good Excellent Good
Stagnant seawater Poor Excellent Moderate
Relative cost High Highest Low

Sizes and welding

Table 5 — Product range and fabrication

Item Detail
Seamless tube OD 6 – 219 mm, WT 1 – 20 mm, ASTM B165
Welded tube OD 12 – 508 mm, WT 0.8 – 8 mm, ASTM B725 / B730
Pipe NPS 1/2 – 12, SCH 10 – 160
Filler ERNiCu-7 / ENiCu-7 matching
Heat input Low; 0.5 – 1.5 kJ/mm
Preheat / PWHT None; stress relief only for anhydrous ammonia service
Post-weld cleaning Pickle and passivate; remove all heat tint

Where Monel 400 is used

HF alkylation

Acid lines, coolers and settlers in hydrofluoric acid alkylation units, where no stainless survives.

Marine pump shafts

Shafts and sleeves in seawater pumps, where the alloy resists erosion and galvanic corrosion.

Caustic handling

Caustic soda evaporators and concentrators, where stainless suffers stress corrosion cracking.

Heat exchanger tube

Seawater and brine exchangers with high flow velocity, where 90-10 CuNi is not corrosion-resistant enough.

Valve trim

Seats, stems and discs in seawater and acid service, often as a solid or weld overlay.

Fasteners

Marine and chemical bolting where stainless galls and galvanic corrosion is a problem.

Frequently asked questions

Is Monel 400 suitable for seawater?

Only in flowing seawater. It resists pitting when velocity is above about 1 m/s; in stagnant or polluted seawater it pits and crevices badly. For stagnant seawater, 625 or a super duplex is the better choice.

Why is Monel 400 used for hydrofluoric acid?

Because it forms a protective fluoride film that is stable in HF across the full concentration range, and it does not catalyse the polymerisation reactions that stainless steels do. It is the reference material for HF alkylation equipment.

Can Monel 400 be hardened by heat treatment?

No. It is a solid-solution alloy and is strengthened only by cold work. Annealing at 870–980 °C softens it. If higher strength is needed, Monel K500 (N05500) is the age-hardenable version.

Is 400 the same as Monel K500?

No. K500 is N05500 with aluminium and titanium added, age hardened to about 790 MPa yield. It is used for pump shafts and valve stems where 400 is too soft, but it is more sensitive to stress corrosion in HF.

What is the maximum temperature?

About 480 °C in air. Above that oxidation becomes rapid, and in sulphur-bearing atmospheres the limit is much lower because of sulphidation. It is not a high-temperature alloy despite the nickel content.

Can Monel 400 be welded?

Yes, with ERNiCu-7 filler and low heat input. The alloy is hot-short if overheated, so keep interpass below 150 °C and avoid excessive heat input. Stress relief is only needed for anhydrous ammonia service.

Does it suffer stress corrosion cracking?

Not in chlorides, which is one reason it is used in marine service. It can crack in anhydrous ammonia and in some mercury-containing environments, and it is susceptible to hydrogen embrittlement in severe cathodic conditions.

What is the minimum order and lead time?

200 kg per size for seamless tube; welded tube from 500 kg. Lead time is 25–40 days depending on size. PMI and third-party inspection add about a week.

Send the medium and the velocity. Monel 400 and 625 both handle seawater, but only one of them handles HF — and only one of them handles stagnant seawater. The quotation will state the grade and the standard.
Request a quote
WhatsApp

Related products

All nickel alloy tube and pipe · Guide: 625, 825, 400 and C276 — which nickel alloy for which medium

Also in this range: Inconel 625 (2.4856) pipe · 904L (1.4539) stainless pipe · F55 (1.4501) super duplex · aerospace stainless tube.

Request a quotation

Give us the form, size, wall, quantity, medium, concentration, temperature, aeration and flow velocity. The last two decide whether Monel 400 is right for seawater.

    Your Name *

    Your Email *

    Company Name

    Phone / WhatsApp *

    Grade & Standard (e.g. ASTM A106 Gr.B, EN 10216-2 P265GH)

    Size, OD × WT (e.g. 88.9 × 5.49 mm)

    Quantity & Unit (e.g. 500 m / 20 t)

    Destination Port

    Drawing or Datasheet (pdf, dwg, step, xlsx; max 5 MB)

    Further Information