Project Description

Inconel 625 N06625 2.4856 nickel chromium iron alloy pipe and tube, pickled finish
N06625 / 2.4856UNS and EN
58% minnickel
8 – 10%molybdenum
415 / 827 MPayield / tensile
980 °Cservice ceiling
OD 6 – 219 mmtube range
MOQ 200 kg per size
Lead time 30–45 days
Third party SGS / BV / TUV
Quote within 24 hours
Certificate EN 10204 3.1 + PMI
Need 625 for high temperature or seawater? Send the service temperature, medium and size — 625 and 825 are not interchangeable and the price difference is large.
Get a quote

Inconel 625 — UNS N06625, W.-Nr. 2.4856 — is a nickel-chromium-molybdenum alloy strengthened by niobium and tantalum rather than by heat treatment. That single design choice explains most of its behaviour: it stays strong from cryogenic temperature to 980 °C, it cannot be hardened or softened by heat treatment after welding, and it tolerates the thermal cycling that would crack a precipitation-hardened alloy. The molybdenum gives it resistance to chlorides and reducing acids, the chromium gives oxidation resistance, and the niobium provides the creep strength that keeps it in jet engine ducting and refinery flare lines. It is also the filler metal of choice for welding 9% nickel steel and duplex stainless, which is why 625 filler sells in a different market from 625 tube.

Chemistry

Table 1 — Chemical composition, ASTM B444 / EN 2.4856 (%, limits)

Element Requirement Function
Nickel 58.0 min Base; austenitic structure and corrosion resistance
Chromium 20.0 – 23.0 Oxidation resistance and passivity
Molybdenum 8.0 – 10.0 Chloride pitting and reducing acid resistance
Niobium + tantalum 3.15 – 4.15 Strengthening and creep resistance; stabilises carbon
Iron 5.0 max Residual
Carbon 0.10 max Kept low for weldability and toughness
Manganese 0.50 max Residual
Silicon 0.50 max Residual
Aluminium 0.40 max Residual; also oxide dispersion in powder metallurgy grades
Titanium 0.40 max Residual
Cobalt 1.0 max Residual
Phosphorus / sulphur 0.015 / 0.015 max Restricted for weldability

Mechanical properties

Table 2 — Room-temperature requirements, annealed

Property Requirement Note
Yield, 0.2% 415 MPa min Annealed condition
Tensile 827 MPa min —
Elongation in 50 mm 30% min —
Hardness ≤ 30 HRC typical Cold worked tube runs higher; state the limit if NACE applies
Solution anneal 1,090 – 1,200 °C, water quench Required after cold work for corrosion service
Creep rupture To 980 °C The reason it is used in hot ducting

Corrosion and high temperature

Table 3 — Service map

Duty 625 performance Comment
Seawater, including stagnant Excellent No pitting or crevice attack at ambient; used for submarine and offshore components
Chloride SCC Immune in practice Nickel content above 58% puts it outside the austenitic cracking range
Oxidation in air Good to 980 °C continuous Above that, oxide spalling begins
Hydrochloric acid Moderate Better than 904L; not for concentrated hot HCl
Sulphuric acid Moderate to good Depends on concentration and temperature
Flue gas and sulphidation Good Refinery flare tips and ducting
Hydrofluoric acid Good, with limits Monel 400 is often better and cheaper for HF

625 against 825 and 800H

Table 4 — Nickel alloy selection

625 (N06625) 825 (N08825) 800H (N08810)
Nickel 58 min 38 – 46 30 – 35
Chromium 20 – 23 19.5 – 23.5 19 – 23
Molybdenum 8 – 10 2.5 – 3.5 —
Strengthening Nb + Ta in solid solution Ti-stabilised Ti-stabilised, coarse grain for creep
Yield 415 MPa 240 MPa 180 MPa
Best at Seawater, high temperature, chlorides Sulphuric and phosphoric acid with chlorides Creep strength to 1,100 °C
Relative cost Highest Lower Lower

Sizes and forms

Table 5 — Product range

Form Range Standard
Seamless tube OD 6 – 219 mm, WT 1 – 20 mm ASTM B444 / B829
Welded tube OD 12 – 508 mm, WT 0.8 – 8 mm ASTM B704 / B705
Pipe NPS 1/2 – 12, SCH 10 – 160 ASTM B444 / B705
Length 3 – 12 m —
Surface Pickled, bright annealed, or ground —
Fittings Butt weld fittings in matching grade B366

Welding and fabrication

Table 6 — Welding parameters

Parameter Recommendation
Filler ERNiCrMo-3 (matching), or ENiCrMo-3 for SMAW
Heat input Low; 0.5 – 1.5 kJ/mm, stringer beads
Interpass ≤ 150 °C
Preheat / PWHT None; the alloy is not hardenable and PWHT is not applicable
Shielding Argon, or argon + helium; purge the root
Post-weld Pickle and passivate; remove all heat tint before corrosive service
Machining Carbide tooling, low speed, high feed, rigid set-up; work hardening is severe

Where 625 is the right answer

Seawater piping

Offshore seawater systems, submerged components and heat exchanger tube where copper-nickel and super duplex both fall short.

Flare and vent systems

Flare tips, risers and ducting that see 900 °C plus sulphidation, where 800H lacks the corrosion resistance.

Chemical plant

Reactors and piping in mixed acid service with chlorides, where 904L corrodes.

Nuclear components

Reactor internals and control rod drive mechanisms, where the alloy’s low activation and corrosion resistance are both required.

Bellows and expansion joints

Thin-wall 625 for high-temperature bellows, where fatigue and oxidation act together.

Welding consumables

625 filler for 9% nickel, duplex and dissimilar joints — a different market from tube but the same heat.

Frequently asked questions

Is Inconel 625 the same as Incoloy 825?

No. 625 is N06625 / 2.4856 with 58% nickel and 8–10% molybdenum; 825 is N08825 / 2.4858 with 38–46% nickel, 3% molybdenum and titanium stabilisation. The material numbers differ by one digit and the alloys differ in corrosion performance and price.

Can 625 be heat treated to increase strength?

No. It is strengthened by solid solution and by the niobium-tantalum addition, not by precipitation hardening. Cold work raises strength; annealing at 1,090–1,200 °C restores the soft condition. There is no ageing treatment.

What is the maximum service temperature?

About 980 °C continuous in air for oxidation resistance, and lower when the environment is sulphidising. It retains useful creep strength to that temperature, which is why it is used in exhaust and flare systems where stainless steels creep.

Is 625 suitable for sour service?

Yes, in the annealed condition with hardness controlled, and it is listed in NACE MR0175 / ISO 15156. Cold worked tube may exceed the hardness limit, so state the sour duty and the acceptable hardness at enquiry.

Why is 625 used as a welding filler?

It tolerates dilution from the base metal, keeps toughness at cryogenic temperature, and does not form brittle phases in the weld. That is why it is the standard filler for 9% nickel steel and for dissimilar joints between stainless and carbon steel.

Can 625 be machined?

Yes, but it work-hardens rapidly. Use carbide tooling, low surface speed, high feed and a rigid set-up, and never let the tool rub. A dull tool will harden the surface and ruin the next pass.

What is the difference between 625 tube and 625 filler?

Same alloy family, different product form and different specification. Tube is certified to ASTM B444 or B704 with dimensional and pressure requirements; filler is certified to AWS A5.14 with a chemistry and deposit test. They are not interchangeable paperwork.

What is the minimum order and lead time?

200 kg per size for seamless tube; welded tube from 500 kg. Lead time is 30–45 days depending on size and whether the mill has the heat. PMI and third-party inspection add about a week.

Send the medium and the temperature. 625 is the answer for seawater and 980 °C, not for every aggressive duty — 825 or 904L is often cheaper and adequate. The quotation will state the grade and the standard.
Request a quote
WhatsApp

Related products

All nickel alloy tube and pipe · Guide: 625, 825, 400 and C276 — which nickel alloy for which medium

Also in this range: Monel 400 (2.4360) pipe · 904L (1.4539) stainless pipe · F55 (1.4501) super duplex · aerospace stainless tube.

Request a quotation

Give us the form, size, wall, quantity, medium, concentration, temperature and whether NACE applies. State the standard (B444, B704, B705) if the drawing names one.

    Your Name *

    Your Email *

    Company Name

    Phone / WhatsApp *

    Grade & Standard (e.g. ASTM A106 Gr.B, EN 10216-2 P265GH)

    Size, OD × WT (e.g. 88.9 × 5.49 mm)

    Quantity & Unit (e.g. 500 m / 20 t)

    Destination Port

    Drawing or Datasheet (pdf, dwg, step, xlsx; max 5 MB)

    Further Information