Project Description

Lead time 20–30 days
Welded cold reduced
Quote within 24 hours
Lengths 6 m or cut
ASTM A554 is the welded mechanical tube specification: stainless tube made from flat strip, welded without filler metal, and supplied as-welded or cold-reduced, in round, square, rectangular and special sections up to 16 inch outside dimension. It exists for structural, ornamental and exhaust work, where mechanical properties, appearance or corrosion resistance matter but pressure containment does not. That last point is the one to remember — A554 carries no pressure rating, and a tube that looks identical to an A269 or A312 product is not certified for pressure service. What it does carry is a shape range those specifications do not cover, plus surface finishes from mill to 400 grit, and a wall tolerance that determines how the corners of a square section behave when it is bent.
Shapes and size range
Table 1 — What the specification covers
| Shape | Typical range | Measured on | Note |
|---|---|---|---|
| Round | 12.7 – 406.4 mm OD | Outside diameter | Above 16 in it is normally A312 pipe |
| Square | 10 × 10 – 150 × 150 mm | Outside dimension, flat to flat | Corner radius grows with wall |
| Rectangular | 20 × 10 up to 200 × 100 mm | Outside dimensions | Aspect ratio above 3:1 distorts on bending |
| Special sections | To drawing | Profile | Roll-formed and welded; needs a tooling order |
| Wall thickness | 0.51 mm (0.020 in) minimum | Wall | Thinner is possible in round sections by agreement |
Grades
Table 2 — Mechanical properties
| Grade | Tensile min | Yield min | Elongation | Use it when |
|---|---|---|---|---|
| 304 | 515 MPa | 205 MPa | 35% | General structural and ornamental, indoor and dry |
| 304L | 485 MPa | 170 MPa | 35% | The tube will be welded after delivery and cannot be annealed |
| 316 | 515 MPa | 205 MPa | 35% | Coastal, marine and chloride-bearing atmospheres |
| 316L | 485 MPa | 170 MPa | 35% | Exhaust, chemical and food-adjacent service with welding |
| 201 | 655 MPa | 260 MPa | 35% | Dry indoor frames where cost matters more than corrosion |
201 is a manganese-substituted grade: stronger and cheaper, noticeably less corrosion resistant. It is common in furniture and shopfitting and it will discolour outdoors. If the part is exposed to weather, 304 is the floor, not 201.
Surface finish
The finish is usually the reason a customer specifies A554 rather than A269. It is also the parameter most often described vaguely on an order — “polished” is not a specification.
Table 3 — Finish options and where each one is accepted
| Finish | Typical Ra | Appearance | Use it for |
|---|---|---|---|
| Mill / as-welded | Ra 1.6 – 3.0 µm | Grey, visible weld line on the face | Concealed structure, exhaust internals |
| Pickled and passivated | Ra 1.6 – 2.5 µm | Uniform matt grey | Outdoor structure where appearance is not critical |
| 180 grit polished | Ra 0.8 µm | Fine directional grain | The general architectural standard |
| 240 grit polished | Ra 0.5 µm | Softer grain | Visible handrails and trim |
| 320 – 400 grit | Ra 0.3 – 0.4 µm | Near-mirror with fine grain | Shopfronts, displays, appliance trim |
| Mirror (buff) | Ra 0.1 µm and below | Reflective | Decorative; shows every handling mark |
Polishing removes the weld line only if it is done after welding and if the wall is thick enough to lose a few hundredths of a millimetre. On thin wall square tube, polishing the weld flat can take the wall below tolerance — state the finish and let us confirm what is achievable at that wall.
Tolerances
Table 4 — What to hold the supplier to
| Parameter | Typical tolerance | Why it matters |
|---|---|---|
| Outside dimension, round | ±0.13 mm under 25 mm, ±0.25 mm above | Determines whether a fitting or cap will seat |
| Outside dimension, square / rectangular | ±0.20 mm | Shows up as a visible step at a mitred joint |
| Wall thickness | ±10% | Drives weldability and bend radius |
| Corner radius | 1.5 × wall to 2.5 × wall | A sharp corner will not take a bend without cracking |
| Out-of-round (OR) | Within the OD tolerance band | Excessive OR jams in a sleeve or a clamp |
| Squareness of cut | 1° maximum | A skewed end shows at every welded joint |
| Straightness | 1 mm per metre | Long handrails and frames accumulate the error |
Where A554 tube is used
Handrails and balustrades
Round and square sections, 180 or 240 grit, in 304 for inland and 316L within a few kilometres of the coast.
Shopfronts and displays
Square and rectangular sections polished to 320–400 grit, where the reflection is the design.
Exhaust systems
409 and 439 for automotive, 304 or 316L for marine and heavy duty. Wall thickness and bend radius decide the grade.
Furniture frames
Thin wall square tube, often 201, bent and welded. Cost drives the grade and the environment decides whether that is acceptable.
Food industry frames
Conveyor frames and guards around a hygienic line, where the product never touches the tube but washdown does.
Architectural cladding
Rectangular sections used as mullions and trim, where straightness over 6 m matters more than wall thickness.
Frequently asked questions
Can A554 tube be used for pressure?
No. It carries no pressure rating. For pressure duty the correct specification is A269 for general service or A312 for pipe sizes; a tube that looks identical is not certified for the same duty.
What does “OR” mean on the drawing?
Out-of-round: the difference between the largest and smallest outside diameter on a round section, or the deviation of a square section from true. It is normally held within the outside dimension tolerance band, and tighter on request.
Is the weld visible?
On mill finish, yes. On polished tube the weld is removed during polishing, provided the wall is thick enough to allow it. On square tube the weld sits at the corner radius and is less visible in the first place.
Can you supply cut lengths?
Yes from 300 mm upwards. Cut ends are deburred; squareness is held to about 1°, and tighter if the tube will be mitred rather than welded square.
304 or 316L for an outdoor handrail?
304 inland, 316L within roughly 5 km of the coast or where de-icing salt is used. Tea staining on 304 near the sea is not a manufacturing defect, it is the grade being wrong for the environment.
What is the minimum wall for a bent section?
It depends on the bend radius rather than the wall alone. As a guide, a centreline radius below 3 × the outside dimension needs either a thicker wall or a mandrel bend. Tell us the bend and we will advise on the wall.
Is the tube solution annealed?
A554 permits as-welded supply, and that is what most ornamental material is. Where corrosion resistance at the weld matters, specify annealed or cold-reduced-and-annealed; it costs more and it is a different product.
What is the minimum order and lead time?
500 kg per size and shape. Lead time is 20–30 days; special sections and mirror polish run longer, and a new roll set for a non-standard section adds two to three weeks.
Request a quote
Related products
ASTM A270 Sanitary TubeHygienic finish for food and dairy
20Cr13 / 420 TubeMartensitic grade for hardened parts
420 / SUS420J1 PipeCutlery and blade grade
410 / 410L TubeLower carbon martensitic
2205 Duplex TubeChloride service beyond 316L
All stainless steel tube — austenitic, martensitic and duplex · Guide: NACE MR0175 sour service requirements
Request a quotation
Tell us shape, outside dimension, wall, grade, finish and quantity. We reply within 24 hours with price, lead time and what the finish will look like at that wall.