Project Description

ASTM A553 9% nickel quenched and tempered steel plate for cryogenic LNG tanks
9% Ni / 8% NiType I and Type II
585 MPayield, Type I
−196 °Cimpact test temperature
27 JCharpy minimum
Q + Tquenched and tempered
6 – 100 mmthickness range
MOQ 5 tonnes
Lead time 30–45 days
Third party SGS / BV / TUV
Quote within 24 hours
Impact tested at −196 °C every lot
Building an LNG or cryogenic tank? Send thickness, size, design code and impact requirement — A553 and A353 are different heat treatments and cannot be quoted as one grade.
Get a quote

ASTM A553 is the quenched and tempered 9% nickel plate specification for cryogenic service, and it is the material that made large LNG storage tanks economic. At −196 °C ordinary carbon steel is brittle, 304L is expensive and has low strength, and 9% nickel steel holds 585 MPa yield with 27 J Charpy impact at liquid nitrogen temperature. The nickel does two things: it lowers the ductile-to-brittle transition so far that the plate stays tough at −196 °C, and it stabilises the austenite enough that the quench produces a martensitic structure that tempers to a tough, strong plate rather than a brittle one. Type I is 9% nickel, Type II is 8% nickel; they are separate grades with separate property tables and cannot be substituted without a design review.

Type I and Type II

Table 1 — The two A553 types

Type I Type II
Nickel 8.50 – 9.50% 7.50 – 8.50%
Yield, 0.2% 585 MPa min 585 MPa min
Tensile 690 – 825 MPa 690 – 825 MPa
Elongation 18% min 18% min
Impact at −196 °C 27 J min 27 J min
Typical use LNG tanks, cryogenic vessels, the standard grade Same duty where the design allows 8% Ni; less common and narrower availability

Type II is not a cheaper Type I. The nickel range, the heat treatment response and the toughness at −196 °C all differ, and a vessel designed around Type I cannot be switched to Type II on price. If a supplier offers “9% Ni” without stating the type, ask for the certificate before the plate is cut.

Chemical composition

Table 2 — Chemical requirements, heat analysis (%)

Element Type I Type II
Carbon 0.13 max 0.13 max
Manganese 0.90 max 0.90 max
Silicon 0.35 max 0.35 max
Phosphorus 0.035 max 0.035 max
Sulphur 0.035 max 0.035 max
Nickel 8.50 – 9.50 7.50 – 8.50
Molybdenum 0.10 max 0.10 max
Chromium 0.25 max 0.25 max
Copper 0.35 max 0.35 max
Vanadium 0.05 max 0.05 max

Heat treatment: the part that decides the properties

Table 3 — Quench and temper cycle

Step Temperature Medium Purpose
Austenitizing 800 – 830 °C — Solution treatment; dissolves carbides and produces austenite
Quench To below 100 °C Water, agitated Transforms to martensite; the fast quench is what gives the toughness
Tempering 540 – 600 °C Air Tempers the martensite, raises toughness, keeps strength above 585 MPa
Cooling after temper Air or water — Avoid slow cooling through the temper embrittlement range

Under-tempering leaves the plate hard and the Charpy values scatter; over-tempering drops the yield below 585 MPa and the plate is rejected on tensile. The window is narrow, which is why 9% Ni plate is bought from mills that do it routinely rather than from a general plate mill on a best-effort basis.

Impact toughness at −196 °C

Table 4 — Charpy V-notch requirements

Property Requirement Test detail
Test temperature −196 °C Liquid nitrogen bath
Average of three specimens 27 J min Transverse direction, standard 10 × 10 mm
Single specimen minimum 20 J One value may fall below the average but not below this
Sub-size specimens Proportional values For plate under 12 mm, the values scale with the section
Test frequency Every heat and heat treatment lot Not sampled across lots

A553 against A353

Table 5 — Two 9% nickel routes, not two names for one plate

A553 Type I A353
Nickel 8.50 – 9.50% 8.50 – 9.50%
Heat treatment Quench and temper Double normalize and temper
Yield, 0.2% 585 MPa min 515 MPa min
Tensile 690 – 825 MPa 690 – 825 MPa
Elongation 18% min 20% min
Impact at −196 °C 27 J 27 J
Where it is chosen New LNG tanks and vessels; higher strength Where a quench is not available, or where the design was written around A353

Welding 9% nickel plate

Table 6 — Welding parameters

Parameter Recommendation Why
Filler ENiCrMo-3 (Alloy 625 type) or ENiCrFe-2 Nickel-based filler tolerates the dilution and keeps weld toughness at −196 °C
Preheat None; keep above 15 °C Preheat is not needed and can increase distortion
Heat input 0.5 – 1.5 kJ/mm High heat input coarsens the HAZ and drops toughness
Interpass ≤ 150 °C Protects the HAZ toughness
PWHT Avoid; if required, ≤ 565 °C Above 565 °C the plate tempers further and loses strength
NDE RT or UT on all vertical and circumferential seams Standard for cryogenic containment

Where A553 plate is used

LNG storage tanks

Inner tank plate for full-containment and membrane tanks, where the design temperature is −165 °C and the plate has to stay tough with a large safety margin.

Cryogenic pressure vessels

Liquid nitrogen, oxygen and argon vessels, usually with A553 Type I and a 27 J acceptance at −196 °C.

LNG carrier containment

Secondary barrier and support structures where 9% Ni competes with stainless and aluminium on weight and weld cost.

Air separation plant

Cold box shells and internal supports, where the plate is welded with nickel filler and no PWHT.

Ethylene terminals

−104 °C service, where 9% Ni is often chosen for its strength rather than its ultimate toughness.

Transition joints

Where a 9% Ni vessel connects to a stainless line, the transition is a dissimilar weld that needs its own procedure qualification.

Frequently asked questions

What is the difference between A553 and A353?

Heat treatment and yield. A553 is quenched and tempered with a 585 MPa minimum yield; A353 is double normalized and tempered with a 515 MPa minimum yield. Both are 9% nickel and both are impact tested at −196 °C to 27 J. They are separate specifications and cannot be substituted without a design review.

Can A553 be substituted for A353?

Only with engineering approval. A553 has the higher yield, so the substitution is conservative on strength, but it changes the welding procedure, the heat treatment of the fabrication and the toughness of the HAZ. A vessel designed and qualified around A353 is not automatically acceptable in A553.

Why is 9% nickel used instead of stainless steel?

Strength and cost. 9% Ni gives 585 MPa yield against about 200 MPa for 304L at room temperature, so the plate is thinner, and it costs less per tonne than 304L. For a large LNG tank the saving in plate weight and weld volume is substantial. Below about 500 m³, stainless or aluminium can be competitive.

Is post-weld heat treatment required?

Normally no. PWHT above 565 °C over-tempers the plate and drops the yield below the specification, so the fabrication is designed to avoid it. Where a code requires stress relief, the temperature is capped and the procedure is qualified with impact testing after the cycle.

What filler metal is used?

Nickel-based filler, typically ENiCrMo-3 (Alloy 625 type) or ENiCrFe-2. Matching 9% Ni ferrous filler does not give reliable weld toughness at −196 °C because of dilution and HAZ coarsening.

What thickness range is available?

6 to 100 mm to A553. Above 100 mm the specification does not cover the thickness and a special approval is needed. Below 12 mm, sub-size Charpy specimens are used and the acceptance values scale with the section.

How is the plate tested before shipment?

Tensile and yield per lot, Charpy at −196 °C every heat and heat treatment lot, chemistry on the heat, dimensional check, and UT to ASTM A435 or EN 10160 where specified. The certificate must state the type, because Type I and Type II look identical on the plate.

What is the minimum order and lead time?

5 tonnes for standard thicknesses because of the mill’s minimum heat and heat treatment batch. Lead time is 30–45 days; third-party witness of the −196 °C impact test adds about a week.

State the type and the design code. A553 Type I, Type II and A353 are three different plates with three different property tables. Send thickness, size, quantity and the impact requirement, and the quotation will name the exact grade.
Request a quote
WhatsApp

Related products

All low temperature and cryogenic steel · All pressure vessel plate · Guide: A553 vs A353 — quenched and tempered against double normalized 9% nickel

Also in this range: ASTM A353 9% nickel plate · ASTM A516 vessel plate · 13CrMo4-5 (1.7335) plate.

Request a quotation

Give us the type (A553 Type I or II), thickness, width, length, quantity, design temperature and the impact test requirement. Tell us the welding procedure and whether PWHT is planned — it affects the acceptable delivery condition.

    Your Name *

    Your Email *

    Company Name

    Phone / WhatsApp *

    Grade & Standard (e.g. ASTM A106 Gr.B, EN 10216-2 P265GH)

    Size, OD × WT (e.g. 88.9 × 5.49 mm)

    Quantity & Unit (e.g. 500 m / 20 t)

    Destination Port

    Drawing or Datasheet (pdf, dwg, step, xlsx; max 5 MB)

    Further Information