Project Description

AISI 410 410L 410S stainless steel pipe, 12 percent chromium martensitic and ferritic grades
410 · 410L · 410Sthree variants
10.5 – 13.5%chromium
≤ 217 HBannealed
40 HRC410 hardened
1.4006 / 1.4003EN numbers
EN 10204 3.1mill certificate
MOQ 300 kg per size
Lead time 20–30 days
PMI 100% on every lot
Quote within 24 hours
Condition annealed
Do you need it to harden? Tell us the part — that single answer decides between 410, 410L and 410S.
Get a quote

These three grades share a chromium level around 12% and a price bracket, and are otherwise different materials. AISI 410 is martensitic with 0.08–0.15% carbon: it hardens to about 40 HRC and is the general-purpose 12% chromium grade. 410L is a low-carbon ferritic grade — 1.4003, C below 0.03% — which does not harden at all but welds easily and is used in structural and transport work. 410S is a low-carbon modification of 410 that stays soft, used where the part must be formed and welded rather than hardened. Choosing the wrong one is a common and expensive mistake: a 410S part that was expected to harden will not, and a 410 part that was expected to weld without preheat will crack.

The three variants

Table 1 — What separates them

410 410L 410S
UNS S41000 S41003 S41008
EN 1.4006 1.4003 1.4000
Structure Martensitic Ferritic Ferritic-martensitic (non-hardening)
C 0.08 – 0.15% 0.03% max 0.08% max
Cr 11.5 – 13.5% 10.5 – 12.5% 11.5 – 13.5%
Hardens? Yes, to about 40 HRC No No, in practice
Welds easily? Only with preheat and PWHT Yes Yes

Mechanical properties

Table 2 — Annealed condition, and what 410 gives when hardened

Grade Tensile Yield Elongation Hardness
410 annealed 480 MPa min 275 MPa min 20% min 217 HB max
410 hardened and tempered 620 – 900 MPa 450 – 700 MPa 15% min 35 – 40 HRC
410L 450 MPa min 280 MPa min 20% min —
410S 415 MPa min 205 MPa min 20% min —

The difference between 480 and 415 MPa is not the point — the point is that one of these three will harden and two will not. If the drawing says “410” and the process requires hardening, substituting 410S because it welds more easily will produce a part that cannot be heat treated.

Where each one belongs

410 — cutlery and wear parts

Knife blades, pump shafts and valve trim where 40 HRC and moderate corrosion resistance are both needed.

410 — steam and water service

Turbine blading and condensate piping, where the grade’s resistance to mild oxidation is adequate and the cost matters.

410L — rail and road vehicles

1.4003 is the standard grade for rail wagons, tipper bodies and bus frames — weldable, cheap, resistant enough to atmosphere.

410L — shipping containers

Corrugated side panels and structural sections, where formability and weldability beat hardness.

410S — mining conveyors

Chute liners and conveyor components where the part is welded and must not crack in the heat-affected zone.

None of them — chlorides

All three pit in chloride service. Marine and chemical duty needs 316L or a duplex grade, not a 12% chromium steel.

Frequently asked questions

Can 410 be welded?

Yes, but only with preheat of 150–250 °C and post-weld heat treatment at 650–750 °C. Without both, the heat-affected zone hardens and cracks. If the part must be welded without PWHT, 410L or 410S is the correct choice.

Will 410S harden?

Not usefully. It is a low-carbon modification intended to stay soft so it can be formed and welded. It work-hardens slightly but will not respond to quench and temper the way 410 does.

Is 410L the same as 1.4003?

Yes. 1.4003 is the EN designation for the low-carbon ferritic 12% chromium grade widely used in rail and transport. It is sometimes sold as “410L” although the chemistry differs slightly from the ASTM S41003 specification.

What is the maximum service temperature?

About 700 °C for oxidation resistance in air, but the mechanical properties fall away above 400 °C. For structural or pressure duty, treat 400 °C as the practical limit.

Why does the certificate need PMI?

Because 410, 410S, 420 and 430 look identical and behave completely differently. A 410S substitution on a part designed to harden to 40 HRC passes every dimension check and fails in service.

Is 410 magnetic?

Yes, all three are ferromagnetic — that is a quick way to separate them from 304 or 316 on the shop floor, though not a way to tell them apart from each other.

Can you supply hardened 410?

Yes, quenched and tempered to a stated hardness range. Most buyers take it annealed and harden after machining, because the annealed condition machines far more easily.

What is the minimum order and lead time?

300 kg per size. Lead time is 20–30 days; hardened and tempered material to a specified hardness runs towards the longer end.

Tell us whether the part must harden. That one answer decides the grade, and it is the question that gets missed most often on a 410 enquiry.
Request a quote
WhatsApp

Related products

All stainless steel tube — austenitic, martensitic and duplex · Guide: NACE MR0175 sour service requirements

Request a quotation

Tell us which variant, OD, wall, condition and quantity — and whether the part will be hardened or welded. We reply within 24 hours with price and lead time.

    Your Name *

    Your Email *

    Company Name

    Phone / WhatsApp *

    Grade & Standard (e.g. ASTM A106 Gr.B, EN 10216-2 P265GH)

    Size, OD × WT (e.g. 88.9 × 5.49 mm)

    Quantity & Unit (e.g. 500 m / 20 t)

    Destination Port

    Drawing or Datasheet (pdf, dwg, step, xlsx; max 5 MB)

    Further Information