Project Description

2304 S32304 1.4362 duplex stainless steel pipe and tube, pickled finish
1.4362 / S32304EN and UNS
400 MPayield, 0.2%
PREN ≈ 25pitting resistance
3.0 – 5.5%nickel
OD 6 – 219 mmround tube
Square / recthollow section to order
MOQ 500 kg per size
Lead time 20–30 days
Third party SGS / BV / TUV
Quote within 24 hours
Certificate EN 10204 3.1
Comparing 2304 with 2101 or 2205? Send the chloride level, temperature and wall — the three grades differ by 10 PREN points and twice the nickel cost.
Get a quote

2304 is the lean duplex grade that sits between 2101 and 2205: S32304 in UNS, 1.4362 in EN, about 23% chromium, 4% nickel and 0.15% nitrogen. It gives roughly double the yield of 316L, better chloride stress corrosion resistance than any austenitic grade, and enough toughness to weld without the strict heat input discipline that 2205 demands. The compromise is pitting resistance — PREN 25 against 35 for 2205 — so it suits chloride levels up to a few hundred ppm and temperatures up to about 80 °C, not seawater. It is the grade to choose when 316L is marginal and 2205 is more than the duty needs.

Chemistry

Table 1 — Chemical composition (%, typical specification limits)

Element 1.4362 / S32304 Effect
Carbon 0.03 max Low enough to weld without carbide precipitation
Chromium 21.5 – 24.5 Corrosion resistance and ferrite
Nickel 3.0 – 5.5 Austenite balance; about half of 2205
Molybdenum 0.05 – 0.60 Pitting resistance; usually around 0.3%
Nitrogen 0.05 – 0.20 Strength and pitting resistance
Manganese 2.5 max Residual austenite former
Copper 0.05 – 0.60 Acid resistance
Silicon 1.0 max Deoxidation

Mechanical properties

Table 2 — Room-temperature requirements

Property Requirement Practical note
Yield, 0.2% 400 MPa min About 2.3× 316L
Tensile 600 MPa min —
Elongation in 50 mm 25% min Lower than austenitic; bend radii must allow for it
Hardness ≤ 290 HBW —
Impact at −40 °C 27 J typical Transition below about −50 °C
Modulus 200 GPa Higher stiffness than 316L, useful in tube bundles

Three lean and standard duplex grades

Table 3 — 2304 against 2101 and 2205

2101 (S32101) 2304 (S32304) 2205 (S32205)
Chromium 21.0 – 22.0 21.5 – 24.5 22.0 – 23.0
Nickel 1.35 – 1.70 3.0 – 5.5 4.5 – 6.5
Molybdenum 0.10 – 0.80 0.05 – 0.60 3.0 – 3.5
Nitrogen 0.20 – 0.25 0.05 – 0.20 0.14 – 0.20
PREN ≈ 26 ≈ 25 ≈ 35
Yield 450 MPa 400 MPa 450 MPa
Chloride limit, ambient ~200 ppm ~300 ppm ~1,000 ppm
Relative cost Lowest Low Highest of the three

PREN 25 against 26 looks like a small difference and in a mixed chloride environment it is not decisive. What actually separates 2101 and 2304 is nickel content and welding behaviour: 2304 is more forgiving on heat input and has better toughness in thick sections, which is why it is preferred for pressure equipment and 2101 for structural sections.

Corrosion performance

Table 4 — Where 2304 is adequate

Duty 2304 Comment
Chlorinated cooling water, ambient Good to about 300 ppm Cl Above that, pitting under deposits becomes likely
Chloride SCC Resistant to about 80 °C The main reason to choose duplex over 316L
Seawater, continuous Not recommended Use super duplex or 6Mo
Dilute sulphuric acid Moderate, to about 5% Above that, 904L
Phosphoric acid Moderate Depends on chloride and fluoride content
Caustic Good to 50% Check SCC at high temperature
Organic acids Good Acetic, formic and citric at moderate temperature

Sizes and forms

Table 5 — Product range

Form Range Tolerance
Seamless round tube OD 6 – 219 mm, WT 1 – 15 mm OD ±0.15 mm, WT ±10%
Welded round tube OD 12 – 508 mm, WT 0.8 – 8 mm OD ±0.20 mm
Square hollow section 20 × 20 – 200 × 200 mm ±0.5 mm
Rectangular hollow section 20 × 40 – 150 × 300 mm ±0.5 mm
Length 3 – 12 m +20 / 0 mm
Surface Pickled, bright annealed, or ground Ra ≤ 1.6 µm pickled

Welding and fabrication

Table 6 — Parameters

Parameter Recommendation
Filler ER2304 for matching joints; ER2209 for higher toughness or dissimilar joints
Heat input 0.5 – 2.0 kJ/mm, wider window than 2205
Interpass ≤ 150 °C
Preheat / PWHT None; PWHT prohibited
Shielding Argon with 2–3% nitrogen for root protection on duplex
Post-weld cleaning Pickle and passivate; wire brushing alone is not enough

Where 2304 is the right answer

Heat exchanger tube

Cooling water exchangers in the 200–300 ppm chloride range, where 316L pits and 2205 is not justified.

Pressure vessels

Chemical and food vessels with chloride-bearing product, where the higher yield reduces wall thickness.

Pulp and paper digesters

White liquor and washing lines where duplex resists erosion corrosion and SCC together.

Desalination

Brine heater and pretreatment stages at moderate chloride levels, with super duplex in the high-chloride stages.

Bridges and structures

Chloride-exposed structural tube where 2101 is unavailable and 2205 is over-specified.

Storage tanks

Chemical storage in coastal locations where external chloride exposure rules out 304 and 316.

Frequently asked questions

Is 2304 the same as 2205?

No. 2304 is S32304 / 1.4362 with PREN about 25 and 4% nickel; 2205 is S32205 / 1.4462 with PREN about 35, 3% molybdenum and 5–6% nickel. 2304 is cheaper and adequate for moderate chlorides; 2205 is the grade for seawater and higher temperatures.

Can 2304 replace 316L?

In chloride service above about 60 °C, yes — that is the main reason to use it. The yield is more than double, so the wall can often be halved, which offsets the higher price per tonne. Check the low-temperature limit and the welding procedure before substituting.

Do you supply 1.4362 hollow sections?

Square and rectangular hollow sections in 1.4362 are made to order from cold formed welded strip, with the grade certificate. They are not seamless, so the pressure rating differs from round seamless tube. Send the section, wall and quantity.

What is the maximum chloride level for 2304?

About 300 ppm at ambient temperature for continuous service, falling as temperature rises. Above 60 °C the safe limit drops sharply. If the chloride level is unknown, ask for the water analysis rather than assuming.

Can 2304 be used at −50 °C?

With impact testing, yes, down to about −50 °C. Below that the ductile-brittle transition makes it unsuitable. Austenitic grades remain the choice for cryogenic service.

Is PWHT permitted on 2304?

No. Heating between 300 and 900 °C forms sigma phase and destroys toughness and corrosion resistance. If stress relief is required by a code, the procedure has to be agreed in advance and verified with impact and corrosion testing.

What is the difference between 2304 and 904L?

Different families. 2304 is duplex with 4% nickel and PREN 25; 904L is super austenitic with 25% nickel, 4.5% molybdenum and PREN 35, and it is the grade for sulphuric and phosphoric acid. 904L is not a duplex and does not have the same yield strength.

What is the minimum order and lead time?

500 kg per size for round seamless tube, 1 tonne for hollow sections. Lead time is 20–30 days; pickled and annealed stock is faster than ground tube.

Send the water analysis with the enquiry. Chloride level and temperature decide whether 2304, 2205 or a super duplex is the correct grade — the price difference between them is large enough to be worth getting right.
Request a quote
WhatsApp

Related products

All stainless steel tube · Guide: 2101, 2304, 2205 and 2507 — which duplex for which chloride level

Also in this range: 2101LDX (1.4162) lean duplex · F55 (1.4501) super duplex · 904L (1.4539) stainless pipe · ASTM A312 TP304 pipe.

Request a quotation

Give us the form, size, wall, quantity, service temperature and chloride level. For heat exchanger duty, include the water analysis — it decides the grade more than the pressure does.

    Your Name *

    Your Email *

    Company Name

    Phone / WhatsApp *

    Grade & Standard (e.g. ASTM A106 Gr.B, EN 10216-2 P265GH)

    Size, OD × WT (e.g. 88.9 × 5.49 mm)

    Quantity & Unit (e.g. 500 m / 20 t)

    Destination Port

    Drawing or Datasheet (pdf, dwg, step, xlsx; max 5 MB)

    Further Information