Project Description

AISI 405 ferritic stainless steel seamless pipe, pickled finish, cut lengths
1.4002EN designation
11.5 – 14.5%chromium
0.08% maxcarbon
0.10 – 0.30%aluminium
415 MPatensile, annealed
OD 6 – 219 mmtube range
MOQ 500 kg per size
Lead time 15–25 days
Third party SGS / BV / TUV
Quote within 24 hours
Certificate EN 10204 3.1
Specifying 405 for a welded assembly? Tell us the welding process and the service temperature — 405 was developed for exactly that, and we will confirm the filler and the condition.
Get a quote

405 is the 12% chromium ferritic stainless steel that does not harden when it is welded. That single property is why it exists. Standard 410 hardens in the heat-affected zone, needs preheat and post-weld heat treatment, and cracks if either is skipped; 405 keeps the carbon at 0.08% maximum and adds 0.10–0.30% aluminium, which suppresses austenite formation enough that the weld zone stays soft and ductile. The trade is strength and hardenability: 405 cannot be quenched and tempered, so it is used annealed, at about 415 MPa tensile, in heat exchanger tubes, vessel internals, trays, ducting and catalytic cracker parts where a 12% chromium steel has to be fabricated on site and then put into service without a heat treatment furnace.

The three 12% chromium grades, side by side

Table 1 — 405 against 410 and 430 — pick by fabrication route, not by corrosion

405 410 430
UNS S40500 S41000 S43000
EN / W.-Nr. 1.4002 / X6CrAl13 1.4006 / X12Cr13 1.4016 / X6Cr17
Chromium 11.5 – 14.5% 11.5 – 13.5% 16.0 – 18.0%
Carbon 0.08 max 0.15 max 0.12 max
Aluminium 0.10 – 0.30% — —
Hardenable No Yes, to 42 HRC No
Weld without PWHT Yes — the design intent No Yes, in thin sections
Corrosion level Similar to 410 Similar to 405 Better; 17% Cr

Chemical composition

Table 2 — Chemical requirements, heat analysis (%)

Element ASTM A268 / A511 EN 10088-2 / 1.4002
Carbon 0.08 max 0.08 max
Manganese 1.00 max 1.00 max
Silicon 1.00 max 1.00 max
Phosphorus 0.040 max 0.040 max
Sulphur 0.030 max 0.030 max
Chromium 11.5 – 14.5 12.0 – 14.0
Aluminium 0.10 – 0.30 0.10 – 0.30
Nickel 0.50 max —

The aluminium range is not a residual — it is the alloying element that makes the grade work. A heat with aluminium below 0.10% will harden in the weld zone like 410, and one above 0.30% becomes difficult to draw and weld cleanly. Check the aluminium on the certificate, not just the chromium.

Mechanical properties

Table 3 — Annealed properties, room temperature

Property Requirement Typical as supplied
Tensile strength 415 MPa min 450 – 520 MPa
Yield strength, 0.2% 170 MPa min 210 – 280 MPa
Elongation in 50 mm 20% min 25 – 32%
Hardness ≤ 179 HBW 150 – 170 HBW
Modulus of elasticity 200 GPa —
Impact, Charpy V Not specified as standard 27 J at 20 °C on request

Corrosion and high-temperature behaviour

405 sits at the same corrosion level as 410: good in atmosphere, fresh water, steam, and many organic and petroleum products; poor in chlorides, seawater and dilute sulphuric acid. The aluminium addition gives it one advantage over 410 — better resistance to oxidation and to sulphidation at elevated temperature, which is why it appears in refinery heater and cracker service where the metal temperature reaches 600–800 °C and the environment is sulphur-bearing.

Table 4 — Service limits

Environment 405 performance Note
Atmosphere, fresh water, steam Good Light staining in coastal atmosphere
Chlorides and seawater Not suitable PREN about 12; pitting and SCC risk
Oxidising sulphidation, 600–800 °C Better than 410 The aluminium effect; used in refinery internals
Scaling in air Good to about 700 °C continuous Above that, 430 or 446 is the better choice
Dilute sulphuric acid Attacked Use 904L or Alloy 20
Caustic soda Acceptable to moderate concentration SCC risk at high concentration and temperature

Welding: the reason to buy 405

Table 5 — Welding parameters

Parameter Recommendation Why
Preheat 100–200 °C, optional Not required for cracking; helps moisture removal and bead shape
Filler ER430 or ER309L Matching ferritic filler gives a soft weld; 309L gives better toughness at the joint
Post-weld heat treatment Not required The low carbon and aluminium keep the HAZ from hardening
Interpass temperature ≤ 300 °C Limits grain growth and sigma formation in thick sections
Shielding gas Argon, or argon + 2% oxygen for TIG Standard austenitic practice applies

405 welds without PWHT, but it is still a ferritic steel: the weld zone grain coarsens and toughness drops. For a vessel in low-temperature service, impact testing of the procedure qualification is still required even though the base metal does not harden.

Dimensions and tolerances

Table 6 — Tube and pipe range

Form Range Tolerance Standard
Seamless tube, cold drawn OD 6 – 114 mm, WT 0.8 – 12 mm OD ±0.10 mm, WT ±10% ASTM A268, A511
Seamless pipe NPS 1/2 – 8, SCH 10 – 160 Per A999 ASTM A268
Welded tube OD 12 – 219 mm, WT 0.8 – 6 mm OD ±0.15 mm ASTM A268
Length 1 – 7 m fixed ±3 mm under 3 m, ±5 mm above —
Surface Pickled, bright annealed, or ground Ra ≤ 1.6 µm pickled —

Standards and equivalents

Table 7 — Cross reference

System Designation Scope
ASTM A268 TP405 / A511 TP405 Seamless and welded ferritic tube
ASTM A240 S40500 Plate and sheet, not tube
EN 1.4002 / X6CrAl13 EN 10088-2 sheet, EN 10216-5 tube on request
JIS SUS405 (G3463 / G4304) Tube and plate
GB 0Cr13Al The Chinese equivalent

Where 405 is the right answer

Heat exchanger tube

Mild process water and oil coolers where the tube is rolled into a carbon steel tubesheet and welded, and PWHT of the assembly is impossible.

Vessel internals

Trays, baffles and supports inside carbon steel vessels, welded on site without a furnace.

Refinery heater parts

Tube supports and hangers in sulphur-bearing service at 600–800 °C, where the aluminium gives an edge over 410.

Catalytic cracker internals

Cyclone parts and liners where erosion resistance and weldability both matter and 410 would need heat treatment.

Ducting and flues

Thin-wall welded duct for flue gas, where the assembly is too large to heat treat and 304 is not justified.

Automotive exhaust

Hangers, flanges and heat shields where 409L is not available and 430 is over-specified on formability.

Frequently asked questions

Why does 405 not harden when welded?

Two reasons: carbon is capped at 0.08%, and 0.10–0.30% aluminium stabilises ferrite so the heat-affected zone does not transform to martensite on cooling. Without the aluminium, a 0.08% carbon 12% Cr steel would still harden slightly in thick sections.

Can 405 be heat treated to increase strength?

No. It is ferritic and not hardenable by quenching. If the part needs 600 MPa or more, use 410 quenched and tempered, or move to a duplex grade. 405 is supplied annealed and stays around 415–520 MPa tensile.

What filler should be used to weld 405?

ER430 or E430 for a matching joint, or ER309L where the joint needs more toughness and the service is not at high temperature. Do not use 308L for high-temperature service — the nickel-rich weld has different thermal expansion and will crack under cycling.

Is 405 the same as 410S?

No, though both are low-carbon 12% Cr. 410S has no aluminium addition and is a low-carbon version of 410; 405 has 0.10–0.30% aluminium specifically to prevent hardening in the weld zone. For welded assemblies 405 is the more forgiving grade.

What is the maximum service temperature for 405?

About 700 °C continuous in air for scaling resistance, and 600–800 °C in sulphidising refinery service where the aluminium oxide layer is protective. Above 800 °C the scale becomes unstable and 446 or a nickel alloy is the correct choice.

Can 405 be used in seawater?

No. At 12% chromium the pitting resistance is far below what chlorides demand, and the ferritic structure is susceptible to stress corrosion cracking in hot chloride service. Use 2205 or a super duplex.

Is 405 magnetic?

Yes, strongly magnetic, like all ferritic grades. It is often chosen for that reason in solenoid and sensor components.

What is the minimum order and lead time?

500 kg per size for standard dimensions. Lead time is 15–25 days depending on size and surface finish; pickled and annealed stock is faster than ground tube. Third-party inspection adds about a week.

Send the fabrication route with the enquiry. Welded or seamless, pickled or bright annealed, and the service temperature — 405 is chosen for its welding behaviour, so the welding process belongs in the quotation.
Request a quote
WhatsApp

Related products

All stainless steel tube · Guide: ferritic stainless steels, and why they are not just cheaper 304

Also in this range: 444 (1.4521) ferritic tube · 10Cr17 / 430 ferritic tube · SUH409L (1.4512) exhaust tube · 410 / 410L / 410S martensitic tube.

Request a quotation

Give us the size, the welded or seamless form, the surface finish and the service environment. We reply within 24 hours with price, lead time and certificate scope.

    Your Name *

    Your Email *

    Company Name

    Phone / WhatsApp *

    Grade & Standard (e.g. ASTM A106 Gr.B, EN 10216-2 P265GH)

    Size, OD × WT (e.g. 88.9 × 5.49 mm)

    Quantity & Unit (e.g. 500 m / 20 t)

    Destination Port

    Drawing or Datasheet (pdf, dwg, step, xlsx; max 5 MB)

    Further Information