A drill pipe is a tube with a tool joint welded on each end. The tube body has to be thinner than the joint — otherwise the pipe cannot be handled, and the weld would sit on a section too thin to carry the make-up torque. That is why the ends are upset: the wall is thickened locally, over a controlled transition length, so there is enough metal to friction weld a joint onto without thickening the whole string.
The upset is not a cosmetic bulge. The transition geometry — how long it is, how gradually the wall grows, whether the thickening is inside, outside or both — determines the fatigue life of the pipe. A short, abrupt transition concentrates stress exactly where the pipe bends in the rotary table. This is the part of the specification that gets argued about most, and the part that is hardest to inspect after the fact.
We supply the upset tube body, not the finished drill pipe. No tool joint, no thread, no weld. If you are the pipe mill or the tool joint supplier, this page is written for you. If you need finished drill pipe, we are the wrong call and we will say so.
Three upset configurations
Table 1 — Upset types and where each is used
| Type | What is thickened | Effect on the bore | Typical use |
|---|---|---|---|
| EU — external upset | Outside diameter only | Bore stays constant | Standard duty, easier to inspect internally |
| IU — internal upset | Inside diameter only | Bore narrows at the ends | Where the outside must stay flush |
| IEU — internal and external | Both, proportioned | Bore narrows slightly, OD grows slightly | Most common for high strength drill pipe |
IEU is the usual choice for S135 and above, because splitting the thickening between inside and outside keeps the transition smoother than putting it all on one surface.
Grades in API 5DP
These are the drill pipe grades. They are not the same list as API 5CT, and the two must not be mixed on a purchase order.
Table 2 — API 5DP mechanical requirements
| Grade | Yield (MPa) | Min tensile (MPa) | Typical depth |
|---|---|---|---|
| E75 | 517–690 | 689 | Shallow, standard duty |
| X95 | 655–862 | 724 | Medium depth |
| G105 | 724–931 | 793 | Deep wells, the workhorse grade |
| S135 | 931–1,138 | 1,000 | Ultra-deep, high torque |
V150 and the SS sour-service series exist but are supplied against a mill-specific specification, not as catalogue items.
When the well is deeper than S135 can carry
P110 and Q125 are API 5CT grades, not API 5DP grades. They are used for drill pipe bodies on a project-specific basis, where the well design demands a yield above S135 and the operator accepts a non-5DP body specification. We supply them as tube bodies to 5CT mechanical properties; we do not describe them as “API 5DP P110 drill pipe”, because that product does not exist in the standard.
Table 3 — High strength options above S135
| Grade | Yield (MPa) | Status | Note |
|---|---|---|---|
| S135 | 931–1,138 | Standard 5DP | Ceiling of the standard grade list |
| P110 | 758–965 | 5CT grade, project basis | Lower yield than S135 but wider toughness allowance |
| Q125 | 862–1,034 | 5CT grade, project basis | Requires a joint and weld procedure qualified for the grade |
Tube body sizes
Table 4 — Standard tube body sizes and wall range
| OD (mm / in) | Wall range (mm) | Upset type | Status |
|---|---|---|---|
| 60.3 / 2⅜ | 5.5–7.1 | EU, IEU | Standard |
| 73.0 / 2⅞ | 5.5–9.2 | EU, IEU | Standard |
| 88.9 / 3½ | 6.5–11.4 | EU, IEU | Standard |
| 101.6 / 4 | 7.1–12.7 | IEU | Standard |
| 114.3 / 4½ | 7.1–12.7 | IEU | Standard |
| 127.0 / 5 | 7.1–12.7 | IEU | Standard |
| 139.7 / 5½ | — | IEU | On request |
| 168.3 / 6⅝ | — | IEU | On request |
Upsetting capacity for this size range tops out at 127 mm OD on the lines we use. 139.7 and 168.3 mm are quoted case by case and are not stock sizes.
The transition is the specification
What the buyer actually needs to control is the upset geometry, not the upset existence. These are the numbers that belong on the drawing.
Table 5 — Upset zone parameters
| Parameter | What it controls | Why it matters |
|---|---|---|
| Upset length | Length of thickened section | Must cover the weld and the joint bevel |
| Transition taper | How gradually the wall changes | Short taper concentrates bending stress |
| Wall increase | Thickness at the upset | Must match the tool joint weld preparation |
| Concentricity at the upset | Bore versus OD at the thickened end | Off-centre upset makes the weld asymmetric |
| Hardness across the transition | Local property change | Upsetting works the metal; hardness has to be checked after |
| Surface condition | Folds or laps in the upset | Folds become crack starters under fatigue |
Which process route the body comes from
Table 6 — Route by size
| Size range | Route | Why |
|---|---|---|
| 60.3–127 mm | Hot rolled + cold drawn + Q&T, then upset | Bore concentricity and wall tolerance are what the upset and weld depend on |
| Above 127 mm | Hot rolled + Q&T, then upset | Cold drawing capacity falls away; wall is thick enough to be self-supporting |
The heat treatment comes before the upset in both routes, and the upset zone is stress relieved afterwards. If the sequence is reversed, the transition cools at a different rate from the body and the hardness profile becomes unpredictable.
Inspection of the upset zone
Table 7 — Test regime for upset tube body
| Test | Coverage | What it catches |
|---|---|---|
| Ultrasonic test, body | 100% | Longitudinal and transverse defects, wall variation |
| Ultrasonic test, upset zone | 100% | Folds and laps created by the upset |
| Magnetic particle, transition | 100% of both ends | Surface and near-surface cracks at the taper |
| Wall thickness, upset | Both ends | Under-thickened sections that would fail the weld |
| Hardness traverse | Across the transition | Hard spots from working or from stress relief |
| Tensile and impact | Per heat | Grade compliance, −20 °C Charpy when specified |
| Straightness | Full length | Bowing that would load the weld in service |
Where the tube body goes next
Friction welded to the tool joint
The upset provides the wall for the weld. The weld procedure is qualified by the pipe mill, not by the tube supplier — but it can only work if the upset geometry is right.
Heat treated after welding
The weld and the upset zone are stress relieved together. Bodies supplied with an inconsistent transition make that post-weld treatment unreliable.
Run in the string
Fatigue, not static load, ends most drill pipe. The transition is where the fatigue crack starts, which is why the taper matters more than the wall number.
Frequently asked questions
What exactly is an upset tube?
A seamless tube with both ends locally thickened by hot upsetting, so that a tool joint can be friction welded onto a section thick enough to carry the load. It is supplied without a joint, without a thread and without a weld.
Why do the ends have to be thickened?
Because the tool joint has a larger OD and a thicker wall than the pipe body. Without an upset, the weld would join a thick part to a thin part and the transition would become the weakest point in the string.
EU or IEU — how do I choose?
EU keeps the bore constant and is easier to inspect internally. IEU splits the thickening between bore and OD, which gives a smoother transition and is the usual choice at S135 and above. The joint weld preparation usually decides it.
Can you supply a P110 drill pipe body?
We can supply the tube body to API 5CT P110 mechanical properties on a project basis. It is not an API 5DP grade, and it should not be described as one. The joint and the weld procedure have to be qualified for the higher strength.
Who cuts the thread and welds the joint?
The pipe mill, not us. We stop at the upset tube body. If you need finished drill pipe with joints and threads, that is a different supply chain and we will tell you so before quoting.
How is the upset transition inspected?
UT over the full upset zone to catch folds, magnetic particle on the taper at both ends, wall thickness at the thickened section, and a hardness traverse across the transition. Visual inspection alone is not sufficient on a fatigue-critical part.
Is the tool joint included?
No. Body only. The commercial reason is simple: joints are a different product with a different qualification route, and mixing them into one purchase order hides which party is responsible for the weld.
How is this different from casing?
Casing is threaded and coupled, and stays in the hole permanently. Drill pipe is a reusable tool that transmits torque and carries drilling fluid. Different standard, different grade list, different failure mode.
Request a quotation
WhatsApp +86 178 7358 1838
Cold Drawn + Q&TSmall OD, thin wall, drawn before quenching.
Small OD Thick Wall60–168.3 mm OD, wall 4.5–18 mm, bore Ra ≤1.6 µm.
P110 Seamless Tube758–965 MPa, wide band, not for sour service.
Q125 Seamless Tube862–1034 MPa, narrow temper window.
Engineering MachineryQ460/E355 weldable, 27SiMn for machined parts.
Sizes above 127 mm are quoted case by case; upsetting capacity, not rolling capacity, is the limit. Related: high pressure gas cylinder tube · alloy steel tube