Project Description

Lead time 20–30 days
Conditions all five available
Quote within 24 hours
Tolerance to EN 10305-1 tables
EN 10305-1 is the part of the EN 10305 series that covers seamless cold drawn tube. What makes it different from a simple dimensional standard is the delivery condition: the same E235 tube can leave the mill at 480 MPa in the hard condition or at 315 MPa annealed, and the difference is not cosmetic — it decides whether the part can be machined without moving, formed without cracking, or welded at all. This page is about the standard itself: the three grades, the five conditions and their mechanical values, and how to pick the right one for a given part. If you are looking for the product rather than the specification, the cold drawn seamless tube page covers sizes, tolerances and process in more depth.
What the standard covers
Table 1 — The EN 10305 series, and which part applies to which product
| Part | Product | Applies here? |
|---|---|---|
| EN 10305-1 | Seamless cold drawn tubes | Yes — this page |
| EN 10305-2 | Welded cold drawn tubes | No — welded, not seamless |
| EN 10305-3 | Welded cold reduced tubes | No — welded, general engineering |
| EN 10305-4 | Seamless cold drawn tubes for hydraulic and pneumatic power systems | No — separate part, adds pressure and cleanliness requirements |
| EN 10305-5 | Welded and cold sized square and rectangular tubes | No — welded, non-round |
| EN 10305-6 | Welded cold drawn tubes for hydraulic and pneumatic power systems | No — welded version of part 4 |
If the drawing says “EN 10305” with no part number, it is incomplete. Part 1 and part 4 have different inspection and cleanliness requirements and are not interchangeable, even though both are seamless cold drawn tube.
Grades and chemistry
Table 2 — Chemical composition (%)
| Grade | Steel number | C max | Si max | Mn max | P max | S max | Al min |
|---|---|---|---|---|---|---|---|
| E215 | 1.0212 | 0.10 | 0.05 | 0.70 | 0.025 | 0.025 | 0.025 |
| E235 | 1.0308 | 0.17 | 0.35 | 1.20 | 0.025 | 0.025 | — |
| E355 | 1.0580 | 0.22 | 0.55 | 1.60 | 0.025 | 0.025 | — |
E215 is the only grade with a mandatory aluminium minimum, because it is the one expected to be formed heavily after delivery — the fine grain is what keeps it from cracking. Manganese rises with the strength grade, from 0.70 to 1.60%.
Mechanical values by delivery condition
This is the table that decides what the part can do. Note that tensile strength between +C and +A spans more than 200 MPa for the same grade — a buyer who orders “E235” without a condition has not actually specified anything.
Table 3 — Mechanical properties by condition
| Grade | Condition | Tensile Rm | Yield ReH | Elongation A min |
|---|---|---|---|---|
| E215 | +C | 430 MPa min | — | 8% |
| E215 | +LC | 380 MPa min | — | 12% |
| E215 | +SR | 380 MPa min | 280 MPa | 16% |
| E215 | +A | 280 MPa min | — | 30% |
| E215 | +N | 290 – 430 MPa | 215 MPa | 30% |
| E235 | +C | 480 MPa min | — | 6% |
| E235 | +LC | 420 MPa min | — | 10% |
| E235 | +SR | 420 MPa min | 350 MPa | 16% |
| E235 | +A | 315 MPa min | — | 25% |
| E235 | +N | 340 – 480 MPa | 235 MPa | 25% |
| E355 | +C | 640 MPa min | — | 4% |
| E355 | +LC | 580 MPa min | — | 7% |
| E355 | +SR | 580 MPa min | 450 MPa | 10% |
| E355 | +A | 450 MPa min | — | 22% |
| E355 | +N | 490 – 630 MPa | 355 MPa | 22% |
Only +SR and +N carry a guaranteed yield in this standard; +C, +LC and +A are specified by tensile and elongation alone. That is not an oversight — in the hard condition the material has no defined yield point, so quoting one would be meaningless.
The five conditions, in plain language
Table 4 — What was done, and what it means for the part
| Code | Last operation | Part behaviour after delivery | Typical use |
|---|---|---|---|
| +C | Final cold draw, no heat treatment | Hardest and strongest; will move when machined; not intended for welding | Finished bore parts, spacers, tubes not machined after delivery |
| +LC | Heat treat, then a light finishing draw | Some forming capacity retained; small bends and flares possible | Parts rolled, crimped or expanded after delivery |
| +SR | Stress relief after final draw | Stable when machined on one side; retains most of the cold-drawn strength | Cylinder barrels, sleeves, anything bored or turned |
| +A | Annealed in controlled atmosphere | Soft, machining-friendly, will not spring back | Heavy machining, subsequent cold forming |
| +N | Normalized in controlled atmosphere | Uniform structure, predictable response to later hardening | Parts that will be hardened or welded after machining |
Choosing the condition — a short selector
Table 5 — Work back from what happens to the part
| If the part will be… | Order | Reason |
|---|---|---|
| Machined on the outside only, finishing pass | +C or +SR | +C is cheaper; use +SR if the wall is thin and distortion matters |
| Bored or honed after delivery | +SR | Removing metal from one side releases drawing stress and bends a +C tube |
| Bent, swaged or expanded | +LC or +A | Needs elongation; +C at 6% will crack |
| Welded into an assembly | +N or +A | +C is explicitly not intended for welding |
| Hardened after machining | +N | Normalized structure gives a predictable hardening response |
| Used as delivered, no further work | +C | Maximum strength at the lowest process cost |
Tolerances
Table 6 — What the standard controls, and where the detail lives
| Parameter | How it is specified | Note |
|---|---|---|
| Outside diameter | Tolerance class against nominal, commonly h9 / h10 / h11 | Class is chosen at order; the full class table is on the cold drawn tube page |
| Inside diameter | Tolerance class where the tube is drawn over a mandrel | Below 40 mm ID the achievable class tightens the price quickly |
| Wall thickness | Percentage of nominal | ±10% is normal commercial practice; tighter by agreement |
| Length | Mill length or cut length | Cut lengths carry a plus tolerance, not a symmetric one |
| Straightness | Deviation per metre | 0.5 mm/m standard; better after straightening and stress relief |
| Surface | As drawn, annealed, or pickled | Stated on the order; +A normally means a bright annealed finish |
Tolerance classes and the ISO 286 values behind them are set out in detail on the cold drawn seamless tube page, together with the size range and the drawing process.
Inspection
Table 7 — Test scope
| Test | Frequency | Recorded |
|---|---|---|
| Chemical analysis | Per cast | EN 10204 3.1 certificate |
| Tensile test | Per lot, per condition | Rm, ReH where applicable, elongation |
| Dimensional | Sample per lot | OD, ID or wall, length, straightness |
| Surface inspection | 100% visual | Defect report if any |
| Eddy current | On request | NDE report |
| Hydrostatic | On request | Test pressure and duration |
Where EN 10305-1 tube is used
Hydraulic cylinder barrels
E235 or E355 in +SR, bored and honed after delivery. The stress relief is what stops the bore going oval when metal is removed.
Automotive suspension parts
E355 in +N or +SR for wishbones, tie rods and axle tubes, where strength per kilogram governs the design.
Shock absorber bodies
E215 in +LC for the outer reservoir, which is rolled and crimped after delivery and must form without cracking.
Bearing rings and spacers
+C with a tight OD class, cut to width and used without machining.
General machined tube
Shaft sleeves, bushes and rollers turned from +A or +SR stock, where the drawn bore saves a boring operation.
Furniture and frame tube
E215 in +A or +N for bending and welding, where formability matters more than strength.
Frequently asked questions
What is the difference between EN 10305-1 and DIN 2391?
EN 10305-1 replaced DIN 2391-1 and -2. The grade names changed from St35, St45 and St52 to E215, E235 and E355, and the delivery condition codes are the same. Old drawings referencing DIN 2391 map directly onto EN 10305-1.
EN 10305-1 or EN 10305-4?
Part 4 is the hydraulic and pneumatic power systems version and adds pressure testing, cleanliness and often tighter tolerances. If the tube becomes a cylinder barrel in a pressure system, the drawing usually means part 4 even when it says part 1 — check before ordering.
Why does the same grade have five different strengths?
Because cold drawing work-hardens the steel and the heat treatments undo it to different degrees. +C is the work-hardened state; +A is fully annealed. Buying “E235” without a condition is an incomplete specification.
Which condition should I order for a honed cylinder barrel?
+SR. Stress relieving after the final draw removes enough residual stress that boring and honing do not distort the bore. A +C tube will machine beautifully and then bend.
Can +C tube be welded?
The standard states that +C is not intended for welding. The work-hardened structure and the absence of any toughness requirement make it a poor choice; order +N or +A if there is a weld in the part.
Is a yield strength guaranteed in the hard condition?
No. +C, +LC and +A are specified by tensile strength and elongation only, because the material has no clearly defined yield point in those conditions. Only +SR and +N carry a minimum ReH.
What does the 3.1 certificate show?
Heat number, chemical analysis, tensile and elongation for the condition supplied, ReH where the condition defines it, and the dimensional inspection result. Eddy current or hydrostatic results are added when those options are ordered.
What is the minimum order and lead time?
500 kg per size and condition. Lead time is 20–30 days; +A and +N need a separate heat treatment cycle and sit at the longer end, while +C can often ship from stock.
Request a quote
Related products
DIN 2391 Precision TubeThe withdrawn predecessor, St35 / St45 / St52
1026 Cold Drawn TubingASTM A519 grade for machined parts
Cold Rolled Seamless TubeBetter surface and concentricity
Chrome Plated Tube+SR base tube, plated for piston rods
AISI 4140 Alloy TubeAlloy route when carbon is not enough
All cold drawn tube — CDS, honed, skived and plated · Guide: cold drawn seamless tube, tolerance classes and delivery conditions
Request a quotation
Give us grade, condition, size, tolerance class and quantity. We reply within 24 hours with price and lead time — and we will query the condition if it does not match what the part will go through.