Project Description

Upset drill pipe tube bodies with thickened ends and machined faces, bundled for shipment
60.3–127 mmOD (2⅜–5 in)
5.5–12.7 mmwall
E75–S135API 5DP grades
P110 / Q125high strength option
8.53–9.45 mRange 2
100% UTupset zone
MOQ 5 tonnes per size
Lead time 25–40 days
Third party SGS / BV / TUV
Quote within 24 hours
Ends upset, ready for friction welding
Tube body only — no tool joint, no thread. We supply the upset tube; the friction weld to the tool joint happens at the pipe mill. Tell us the joint OD and the weld procedure and we will match the upset profile.
Request a quote

A drill pipe is a tube with a tool joint welded on each end. The tube body has to be thinner than the joint — otherwise the pipe cannot be handled, and the weld would sit on a section too thin to carry the make-up torque. That is why the ends are upset: the wall is thickened locally, over a controlled transition length, so there is enough metal to friction weld a joint onto without thickening the whole string.

The upset is not a cosmetic bulge. The transition geometry — how long it is, how gradually the wall grows, whether the thickening is inside, outside or both — determines the fatigue life of the pipe. A short, abrupt transition concentrates stress exactly where the pipe bends in the rotary table. This is the part of the specification that gets argued about most, and the part that is hardest to inspect after the fact.

We supply the upset tube body, not the finished drill pipe. No tool joint, no thread, no weld. If you are the pipe mill or the tool joint supplier, this page is written for you. If you need finished drill pipe, we are the wrong call and we will say so.

Three upset configurations

Table 1 — Upset types and where each is used

Type What is thickened Effect on the bore Typical use
EU — external upset Outside diameter only Bore stays constant Standard duty, easier to inspect internally
IU — internal upset Inside diameter only Bore narrows at the ends Where the outside must stay flush
IEU — internal and external Both, proportioned Bore narrows slightly, OD grows slightly Most common for high strength drill pipe

IEU is the usual choice for S135 and above, because splitting the thickening between inside and outside keeps the transition smoother than putting it all on one surface.

Grades in API 5DP

These are the drill pipe grades. They are not the same list as API 5CT, and the two must not be mixed on a purchase order.

Table 2 — API 5DP mechanical requirements

Grade Yield (MPa) Min tensile (MPa) Typical depth
E75 517–690 689 Shallow, standard duty
X95 655–862 724 Medium depth
G105 724–931 793 Deep wells, the workhorse grade
S135 931–1,138 1,000 Ultra-deep, high torque

V150 and the SS sour-service series exist but are supplied against a mill-specific specification, not as catalogue items.

When the well is deeper than S135 can carry

P110 and Q125 are API 5CT grades, not API 5DP grades. They are used for drill pipe bodies on a project-specific basis, where the well design demands a yield above S135 and the operator accepts a non-5DP body specification. We supply them as tube bodies to 5CT mechanical properties; we do not describe them as “API 5DP P110 drill pipe”, because that product does not exist in the standard.

Table 3 — High strength options above S135

Grade Yield (MPa) Status Note
S135 931–1,138 Standard 5DP Ceiling of the standard grade list
P110 758–965 5CT grade, project basis Lower yield than S135 but wider toughness allowance
Q125 862–1,034 5CT grade, project basis Requires a joint and weld procedure qualified for the grade

Tube body sizes

Table 4 — Standard tube body sizes and wall range

OD (mm / in) Wall range (mm) Upset type Status
60.3 / 2⅜ 5.5–7.1 EU, IEU Standard
73.0 / 2⅞ 5.5–9.2 EU, IEU Standard
88.9 / 3½ 6.5–11.4 EU, IEU Standard
101.6 / 4 7.1–12.7 IEU Standard
114.3 / 4½ 7.1–12.7 IEU Standard
127.0 / 5 7.1–12.7 IEU Standard
139.7 / 5½ — IEU On request
168.3 / 6⅝ — IEU On request

Upsetting capacity for this size range tops out at 127 mm OD on the lines we use. 139.7 and 168.3 mm are quoted case by case and are not stock sizes.

The transition is the specification

What the buyer actually needs to control is the upset geometry, not the upset existence. These are the numbers that belong on the drawing.

Table 5 — Upset zone parameters

Parameter What it controls Why it matters
Upset length Length of thickened section Must cover the weld and the joint bevel
Transition taper How gradually the wall changes Short taper concentrates bending stress
Wall increase Thickness at the upset Must match the tool joint weld preparation
Concentricity at the upset Bore versus OD at the thickened end Off-centre upset makes the weld asymmetric
Hardness across the transition Local property change Upsetting works the metal; hardness has to be checked after
Surface condition Folds or laps in the upset Folds become crack starters under fatigue

Which process route the body comes from

Table 6 — Route by size

Size range Route Why
60.3–127 mm Hot rolled + cold drawn + Q&T, then upset Bore concentricity and wall tolerance are what the upset and weld depend on
Above 127 mm Hot rolled + Q&T, then upset Cold drawing capacity falls away; wall is thick enough to be self-supporting

The heat treatment comes before the upset in both routes, and the upset zone is stress relieved afterwards. If the sequence is reversed, the transition cools at a different rate from the body and the hardness profile becomes unpredictable.

Inspection of the upset zone

Table 7 — Test regime for upset tube body

Test Coverage What it catches
Ultrasonic test, body 100% Longitudinal and transverse defects, wall variation
Ultrasonic test, upset zone 100% Folds and laps created by the upset
Magnetic particle, transition 100% of both ends Surface and near-surface cracks at the taper
Wall thickness, upset Both ends Under-thickened sections that would fail the weld
Hardness traverse Across the transition Hard spots from working or from stress relief
Tensile and impact Per heat Grade compliance, −20 °C Charpy when specified
Straightness Full length Bowing that would load the weld in service

Where the tube body goes next

Friction welded to the tool joint

The upset provides the wall for the weld. The weld procedure is qualified by the pipe mill, not by the tube supplier — but it can only work if the upset geometry is right.

Heat treated after welding

The weld and the upset zone are stress relieved together. Bodies supplied with an inconsistent transition make that post-weld treatment unreliable.

Run in the string

Fatigue, not static load, ends most drill pipe. The transition is where the fatigue crack starts, which is why the taper matters more than the wall number.

Frequently asked questions

What exactly is an upset tube?

A seamless tube with both ends locally thickened by hot upsetting, so that a tool joint can be friction welded onto a section thick enough to carry the load. It is supplied without a joint, without a thread and without a weld.

Why do the ends have to be thickened?

Because the tool joint has a larger OD and a thicker wall than the pipe body. Without an upset, the weld would join a thick part to a thin part and the transition would become the weakest point in the string.

EU or IEU — how do I choose?

EU keeps the bore constant and is easier to inspect internally. IEU splits the thickening between bore and OD, which gives a smoother transition and is the usual choice at S135 and above. The joint weld preparation usually decides it.

Can you supply a P110 drill pipe body?

We can supply the tube body to API 5CT P110 mechanical properties on a project basis. It is not an API 5DP grade, and it should not be described as one. The joint and the weld procedure have to be qualified for the higher strength.

Who cuts the thread and welds the joint?

The pipe mill, not us. We stop at the upset tube body. If you need finished drill pipe with joints and threads, that is a different supply chain and we will tell you so before quoting.

How is the upset transition inspected?

UT over the full upset zone to catch folds, magnetic particle on the taper at both ends, wall thickness at the thickened section, and a hardness traverse across the transition. Visual inspection alone is not sufficient on a fatigue-critical part.

Is the tool joint included?

No. Body only. The commercial reason is simple: joints are a different product with a different qualification route, and mixing them into one purchase order hides which party is responsible for the weld.

How is this different from casing?

Casing is threaded and coupled, and stays in the hole permanently. Drill pipe is a reusable tool that transmits torque and carries drilling fluid. Different standard, different grade list, different failure mode.

Send the upset drawing, not just the OD. Transition length, taper, wall increase and joint weld preparation decide whether the body works. We will confirm the upset profile against our tooling before quoting.
Request a quotation
WhatsApp +86 178 7358 1838

Sizes above 127 mm are quoted case by case; upsetting capacity, not rolling capacity, is the limit. Related: high pressure gas cylinder tube · alloy steel tube

Request a quotation

    Your Name *

    Your Email *

    Company Name

    Phone / WhatsApp *

    Grade & Standard (e.g. ASTM A106 Gr.B, EN 10216-2 P265GH)

    Size, OD × WT (e.g. 88.9 × 5.49 mm)

    Quantity & Unit (e.g. 500 m / 20 t)

    Destination Port

    Drawing or Datasheet (pdf, dwg, step, xlsx; max 5 MB)

    Further Information