Project Description

European and Japanese Standard Boiler Tubes — Hunan Fushun Metal

European and Japanese Standard Boiler Tubes

Product Description

Boiler tubes are primarily used in supercritical or ultra-supercritical boilers for components such as superheaters, reheaters, water walls, and economizers. These tubes require high long-term strength, excellent anti-oxidation and corrosion resistance, as well as good structural stability.

Main Grades or Steel Grades

EN10216-2:

  • P195GH
  • P235GH
  • P265GH
  • 20MnNb6
  • 16Mo3
  • 8MoB5-4
  • 14MoV6-3
  • 10CrMo5-5
  • 13CrMo4-5
  • 10CrMo9-10
  • 11CrMo9-10
  • 20CrMoV13-5-5
  • X11CrMo5+1
  • X11CrMo5+NT1
  • X11CrMo5+NT2
  • X11CrMo9-1+1
  • X11CrMo9-1+NT
  • X10CrMoVNb9-1
  • X20CrNiV11-1

JIS G3454:

  • STPG 370 (STPG 38)
  • STPG 410 (STPG 42)

JIS G3461:

  • STB 35
  • STB 42
  • STB 52

JIS G3462:

  • STBA12
  • STBA13
  • STBA20
  • STBA22
  • STBA23
  • STBA24
  • STBA25
  • STBA26

Standards

  • EN10216-2: Specifies alloy and non-alloy steel tubes for high-temperature service.
  • JIS G3454: Carbon steel tubes for pressure service.
  • JIS G3461: Carbon steel tubes for boilers and heat exchangers.
  • JIS G3462: Alloy steel tubes for boilers and heat exchangers.

Product Features

Boiler tubes often operate under high temperature and pressure conditions. The tubes can experience oxidation and corrosion under the influence of high-temperature flue gas and steam. Therefore, boiler steel tubes must have high long-term strength, excellent anti-oxidation and corrosion resistance, and good structural stability.

Size Range

Outer Diameter: Φ15.88~89mm; Wall Thickness: 2.6~12.5mm

EN and JIS boiler tube data

The same tube can be ordered to EN or to JIS, and the two routes are not interchangeable on paper: EN 10216-2 grades carry elevated-temperature proof strength values that JIS G3461 / G3462 grades do not tabulate. If the design is European, keep the EN grade designation on the purchase order even when the tube is rolled in Asia.

European standard EN 10216-2, test category TC1 or TC2
EN grades P195GH, P235GH, P265GH, 20MnNb6, 16Mo3, 8MoB5-4, 14MoV6-3, 10CrMo5-5, 13CrMo4-5, 10CrMo9-10, 11CrMo9-10, 20CrMoV13-5-5, X11CrMo5+1/+NT1/+NT2, X11CrMo9-1+1/+NT, X10CrMoVNb9-1, X20CrNiV11-1
Japanese standards JIS G3454 (STPG 370, STPG 410); JIS G3461 (STB 35, 42, 52); JIS G3462 (STBA 12, 13, 20, 22, 23, 24, 25, 26)
Outside diameter 15.88 mm – 89 mm
Wall thickness 2.6 mm – 12.5 mm
Delivery condition Normalized, or normalized and tempered for the 9 % Cr grades
Testing TC1: tensile, flattening, leak-tightness. TC2 adds impact testing at the agreed temperature
Certificate EN 10204 3.1; 3.2 with third-party inspection on request

TC1 and TC2 differ only by the impact test, but the price difference is real. Confirm which category the design calls for before quoting — most European boiler orders specify TC2 for the pressure parts and TC1 for supports and non-pressure attachments.