Project Description
European and Japanese Standard Boiler Tubes
Product Description
Boiler tubes are primarily used in supercritical or ultra-supercritical boilers for components such as superheaters, reheaters, water walls, and economizers. These tubes require high long-term strength, excellent anti-oxidation and corrosion resistance, as well as good structural stability.
Main Grades or Steel Grades
EN10216-2:
- P195GH
- P235GH
- P265GH
- 20MnNb6
- 16Mo3
- 8MoB5-4
- 14MoV6-3
- 10CrMo5-5
- 13CrMo4-5
- 10CrMo9-10
- 11CrMo9-10
- 20CrMoV13-5-5
- X11CrMo5+1
- X11CrMo5+NT1
- X11CrMo5+NT2
- X11CrMo9-1+1
- X11CrMo9-1+NT
- X10CrMoVNb9-1
- X20CrNiV11-1
JIS G3454:
- STPG 370 (STPG 38)
- STPG 410 (STPG 42)
JIS G3461:
- STB 35
- STB 42
- STB 52
JIS G3462:
- STBA12
- STBA13
- STBA20
- STBA22
- STBA23
- STBA24
- STBA25
- STBA26
Standards
- EN10216-2: Specifies alloy and non-alloy steel tubes for high-temperature service.
- JIS G3454: Carbon steel tubes for pressure service.
- JIS G3461: Carbon steel tubes for boilers and heat exchangers.
- JIS G3462: Alloy steel tubes for boilers and heat exchangers.
Product Features
Boiler tubes often operate under high temperature and pressure conditions. The tubes can experience oxidation and corrosion under the influence of high-temperature flue gas and steam. Therefore, boiler steel tubes must have high long-term strength, excellent anti-oxidation and corrosion resistance, and good structural stability.
Size Range
Outer Diameter: Φ15.88~89mm; Wall Thickness: 2.6~12.5mm
EN and JIS boiler tube data
The same tube can be ordered to EN or to JIS, and the two routes are not interchangeable on paper: EN 10216-2 grades carry elevated-temperature proof strength values that JIS G3461 / G3462 grades do not tabulate. If the design is European, keep the EN grade designation on the purchase order even when the tube is rolled in Asia.
| European standard | EN 10216-2, test category TC1 or TC2 |
| EN grades | P195GH, P235GH, P265GH, 20MnNb6, 16Mo3, 8MoB5-4, 14MoV6-3, 10CrMo5-5, 13CrMo4-5, 10CrMo9-10, 11CrMo9-10, 20CrMoV13-5-5, X11CrMo5+1/+NT1/+NT2, X11CrMo9-1+1/+NT, X10CrMoVNb9-1, X20CrNiV11-1 |
| Japanese standards | JIS G3454 (STPG 370, STPG 410); JIS G3461 (STB 35, 42, 52); JIS G3462 (STBA 12, 13, 20, 22, 23, 24, 25, 26) |
| Outside diameter | 15.88 mm – 89 mm |
| Wall thickness | 2.6 mm – 12.5 mm |
| Delivery condition | Normalized, or normalized and tempered for the 9 % Cr grades |
| Testing | TC1: tensile, flattening, leak-tightness. TC2 adds impact testing at the agreed temperature |
| Certificate | EN 10204 3.1; 3.2 with third-party inspection on request |